Fabrication of monolithic diamond photodetector with microlenses
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-12-05 |
| Journal | Optics Express |
| Authors | Tianfei Zhu, Zongchen Liu, Zhangcheng Liu, Fengnan Li, Minghui Zhang |
| Citations | 32 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Core Innovation: Fabrication of a monolithic diamond photodetector featuring etched microlens arrays (MLAs) on a single crystal diamond (SCD) surface, integrated with patterned tungsten interdigitated electrodes.
- Key Performance Gain: Achieved a 74.8% increase in photocurrent at 10 V under 220 nm deep-UV illumination compared to a planar reference device.
- Fabrication Approach: Utilized thermal reflow of photoresist to create MLAs on the SCD surface, followed by magnetron sputtering to deposit tungsten (W) electrodes directly on the lens edges and planar regions.
- Mechanism: Improvement is attributed to enhanced light absorption efficiency via light concentration and improved charge collection efficiency at the electrode edges.
- Target Application: Deep-ultraviolet (DUV) and solar-blind photodetection, with a device architecture broadly transferable to other semiconductor photodetector systems.
- Process Flow: Photoresist patterning → thermal reflow → diamond etching → electrode metallization, all on a single monolithic chip.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Photocurrent Enhancement | 74.8 | % | At 10 V under 220 nm UV illumination |
| Applied Bias Voltage | 10 | V | Operating voltage during measurement |
| Illumination Wavelength | 220 | nm | Deep-UV (solar-blind region) |
| Spectral Range Tested | 200 - 600 | nm | Photoresponse sweep |
| Electrode Material | Tungsten (W) | — | Deposited via magnetron sputtering |
| Electrode Geometry | Interdigitated strips | — | One set on MLA edges, one on flat area |
| Lens Fabrication Method | Thermal reflow of photoresist | — | Followed by dry etching into SCD |
| Diamond Type | Single Crystal Diamond (SCD) | — | Monolithic substrate |
| Device Architecture | Metal-Semiconductor-Metal (MSM) | — | Schottky-contact interdigitated layout |
| Lens Diameter (approx.) | 100 | µm | Estimated from figure scale bar |
| Electrode Pitch | 4 - 5 | µm | Finger width/spacing from SEM images |
| Charge Collection Improvement | Significantly higher field at microlens edge | — | Confirmed by 2D electric field simulation |
| Light Absorption Simulation | Higher photon density under MLA | — | Confirmed by optical FDTD/ray-tracing |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Start with an optical-grade single crystal diamond (SCD) wafer with low surface roughness suitable for photolithography.
- Photoresist Patterning: Spin-coat photoresist onto the diamond surface; use a photomask to define circular pads over half the sample area (leaving the other half planar as a control).
- Thermal Reflow: Heat the patterned photoresist above its glass transition temperature to form smooth, dome-shaped microlenses.
- Reactive Ion Etching (RIE): Transfer the curved photoresist profile into the underlying diamond substrate, creating MLAs directly in the SCD.
- Electrode Definition: Perform a second lithography step to open contact windows on the MLA edges and the planar region.
- Magnetron Sputtering: Deposit tungsten (W) as the electrode metal, chosen for its compatibility with diamond processing and high-temperature stability.
- Lift-off / Patterning: Define interdigitated electrode fingers (approx. 4-5 µm pitch) via standard lift-off.
- Electrical & Optical Characterization: Measure I-V curves under 220 nm UV and sweep spectral responsivity from 200 nm to 600 nm; compare microlens vs. planar devices on the same chip.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”| Research Need from Paper | 6CCVD Capability Match |
|---|---|
| High-quality SCD substrate for microlens etching and UV transmission | Optical Grade Single Crystal Diamond (SCD) — available from 0.1 µm to 500 µm thickness with Ra < 1 nm polish |
| Tungsten (W) interdigitated electrodes | Custom Tungsten (W) Metallization — in-house sputtering capability alongside Au, Pt, Pd, Ti, and Cu |
| Precise microlens patterning requiring ultra-flat, defect-free starting surface | Sub-nm polishing (Ra < 1 nm on SCD) — ensures uniform photoresist reflow and clean RIE transfer |
| Plate format for monolithically integrated detector arrays | Custom SCD plates up to 125 mm equivalent (PCD); SCD substrates available in standard and custom dimensions |
| Deep-UV / solar-blind detector development | Engineer-ready SCD and BDD wafers optimized for UV detection, radiation-hard, and high-temperature operation |
| Dicing of small detector pixels / chips | Laser cutting and dicing services for custom chip geometries |
Applicable Materials
For replication or extension of this monolithic diamond photodetector with microlenses, 6CCVD recommends Optical Grade Single Crystal Diamond (SCD) with sub-nanometer surface polish. The ultra-low roughness is critical for uniform photoresist reflow and clean RIE pattern transfer into diamond. For variants requiring a conductive electrode interface or B-doped contact layers, Boron-Doped Diamond (BDD) can be supplied as a companion or epitaxial layer.
Customization Potential
The tungsten interdigitated electrode pattern used in this study is fully supported by 6CCVD’s internal metallization line. We can deposit W, Ti/W, Ti/Pt/Au, or other refractory / noble metal stacks with custom finger widths and pitches down to the micron scale. Combined with our laser cutting and dicing service, we can deliver finished SCD chips in the exact dimensions required for your MSM detector array, with MLA etch-ready or pre-patterned surfaces on request.
Engineering Support
6CCVD’s in-house PhD engineering team can assist with material selection, surface preparation, and metallization stack design for deep-ultraviolet photodetector, solar-blind sensor, and integrated micro-optics projects on diamond. Whether you are scaling up this MLA architecture, moving to a BDD active layer, or exploring new electrode geometries, our team can recommend the optimal SCD grade, thickness, and surface specification for your process.
Call to Action
For custom specifications, metallization stacks, or material consultation on diamond-based UV photodetectors, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
A monolithic diamond photodetector with microlenses is fabricated by etching microlens arrays (MLAs) on single crystal diamond surface and patterning tungsten electrode strips on the edge of these arrays. Firstly, compact MLAs are etched on half of diamond sample surface by thermal reflow method. Secondly, via magnetron sputtering technique, two sets of interdigitated tungsten electrodes are patterned on the sample surface, one set is on the edge of MLAs, the other set is on the planar area. The optoelectronic performances of photodetectors have been investigated and indicated that the photocurrent of microlens photodetector increases by 74.8 percent at 10 V under 220 nm UV light illumination by comparing with that in planar case. Simulations of photodetectors’ electrical and optical properties have been carried out, illustrating an improvement of charge collection ability and light absorption efficiency in microlens case. Furthermore, the present device structure can be extended to other semiconductor photodetectors.