A sp2+sp3 hybridized carbon allotrope transformed from AB stacking graphyne and THD-graphene

MetadataDetails
Publication Date2018-01-01
JournalAIP Advances
AuthorsYu Zhang, Jiacheng Shang, Weida Fu, Li Zeng, Tao Tang
InstitutionsNanchang University
Citations12

New carbon allotropes can be designed by combining sp, sp2 and sp3 three hybridization states. And the hybridization states or coordination numbers of carbon atoms can be changed by applying high pressure on carbon materials. In this study, a common high pressure phase (named as TBBC) transformed from AB-stacking graphyne or THD-graphene is predicted. Its kinetic stability is examined using finite displacement method. We find that the sp2 and sp3 hybridized carbon atoms behave different vibration features at high frequency region. Both graphene-like and diamond-like vibration peaks occurs. Phase transition energy barriers from both graphyne and THD-graphene to TBBC are estimated. Electronic structure calculations show that the TBBC is an indirect semiconductor with a bandgap of 0.66 eV. The ideal tensile strength of TBBC is high in [0001] and [11ĀÆ00] directions, but is weak along [12ĀÆ10] direction.

  1. 2011 - T-carbon: A novel carbon allotrope [Crossref]
  2. 1985 - C60: Buckminsterfullerene [Crossref]
  3. 1991 - Helical microtubules of graphitic carbon [Crossref]
  4. 2010 - Architecture of graphdiyne nanoscale films [Crossref]
  5. 2005 - Two-dimensional atomic crystals [Crossref]
  6. 2004 - Electric field effect in atomically thin carbon films [Crossref]
  7. 2000 - Quantized phonon spectrum of single-wall carbon nanotubes [Crossref]
  8. 1995 - A carbon nanotube field-emission electron source [Crossref]
  9. 2011 - Graphdiyne: A versatile nanomaterial for electronics and hydrogen purification [Crossref]
  10. 2012 - Selective hydrogen purification through graphdiyne under ambient temperature and pressure [Crossref]