Characterization of high-transconductance long-channel hydrogen-terminated polycrystal diamond field effect transistor
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Acta Physica Sinica |
| Authors | Zhang Jin-Feng, Yang Peng-Zhi, Ren Ze-Yang, Jincheng Zhang, Xu Shengrui |
| Citations | 2 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Device Architecture: Long-channel hydrogen-terminated polycrystalline diamond (PCD) MESFET utilizing a self-aligned 4 µm aluminum gate, fabricated on a 10 mm × 10 mm × 0.3 mm (001) PCD substrate.
- Peak Transconductance: Achieves a maximum external transconductance (gm) of 32 mS/mm with an intrinsic gm0 of 58 mS/mm, demonstrating exceptional signal amplification capability.
- Broad High-gm Operating Window: Sustains transconductance above 90% of its peak across a wide 3 V gate bias range (VGS = −2 V to −5 V), ideal for high-linearity RF power amplifiers.
- Low On-Resistance: Delivers Ron of 37.85 Ω·mm and saturation drain current (IDsat) of 160 mA/mm, outperforming comparable long-channel diamond FETs.
- Channel Carrier Density: Achieves a high hole sheet density of 1.56 × 1013 cm−2 under the gate, supported by low sheet resistance (5.71 kΩ/sq) and low Ohmic contact resistance (5.52 Ω·mm).
- Stable Effective Mobility: Maintains near-constant effective hole mobility of ~170 cm2/(V·s) across the high-transconductance bias range, preventing typical high-field mobility degradation.
- Process Highlights: Surface hydrogenation via MPCVD (H2 plasma, 500 sccm, 80 mbar, 2 kW), 100 nm Au thermal evaporation for Ohmic contacts, and selective O2 plasma oxidation for device isolation.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Gate Length (LG) | 4 | µm | Long-channel MESFET geometry |
| Gate Width (WG) | 50 | µm | Single-finger Al gate |
| Saturation Drain Current (IDsat) | 160 | mA/mm | Measured at VGS = −5 V |
| On-Resistance (Ron) | 37.85 | Ω·mm | Extracted from VDS < 0.1 V I-V data |
| Max External Transconductance (gm) | 32 | mS/mm | Peak at VGS = −3.5 V |
| Max Intrinsic Transconductance (gm0) | 58 | mS/mm | Calculated after RS de-embedding |
| High-gm Voltage Range (≥90% peak) | 3 | V | VGS = −2 V to −5 V |
| Threshold Voltage (VTH) | 1.4 | V | Extracted from transfer curve @ VDS = −9 V |
| Flat-Band Voltage (VFB) | 1.67 | V | Extracted from C-V characteristics |
| Ohmic Contact Resistance (RC) | 5.52 | Ω·mm | Transmission line model (TLM) |
| Specific Contact Resistivity (ρC) | 5.30 × 10−5 | Ω·cm2 | TLM extraction |
| Hydrogen-Terminated Sheet Resistance | 5.71 | kΩ/sq | Material-level measurement |
| Channel Sheet Resistance (Rsh_ch) | 2.42 | kΩ/sq | At VGS = −5 V (gate-induced accumulation) |
| Hole Sheet Density (pch) | 1.56 × 1013 | cm−2 | Integrated from C-V at VGS = −5 V |
| Effective Mobility (µeff) | ~170 | cm2/(V·s) | Constant across high-gm range |
| Max Gate Capacitance (Cox) | 0.374 | µF/cm2 | Measured at 1 MHz |
| Al2O3 Interfacial Layer Thickness | ~8.3 | nm | Calculated from C-V, εr = 3.5 |
| Source/Drain Series Resistance (RS/RD) | 14.08 | Ω·mm | Includes RC + access region |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Commercial 10 mm × 10 mm × 0.3 mm (001) polycrystalline diamond from Element Six; sequential ultrasonic cleaning in acetone, anhydrous ethanol, and deionized water (15 min each).
- Hydrogen Plasma Treatment: MPCVD hydrogenation at H2 flow = 500 sccm, pressure = 80 mbar, microwave power = 2 kW; cooled to room temperature in H2 ambient to generate C-H surface termination.
- Surface Conditioning: Air exposure for several hours to form an adsorbed hole-inducing layer (containing OH−, HCO3−).
- Ohmic Contact Formation: Thermal evaporation of 100 nm Au; photolithographic patterning and KI/I2 wet etching to define source/drain electrodes.
- Device Isolation: Low-power O2 plasma treatment (10 min) converting exposed H-terminated regions to insulating O-terminated surfaces.
- Gate Definition: Selective Au wet etching (lateral undercut defining LG = 4 µm gap); thermal evaporation of 100 nm Al; lift-off process for self-aligned gate formation.
- Electrical Characterization: Keithley 4200 semiconductor parameter analyzer for DC I-V and 1 MHz C-V measurements.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials: This research relies on high-quality Optical Grade or Electronic Grade Polycrystalline Diamond (PCD) with grain sizes exceeding 100 µm and a polished surface suitable for micron-scale lithography. 6CCVD supplies PCD substrates in standard thicknesses (0.1 µm-500 µm freestanding, or up to 10 mm substrate-backed), with surface roughness polished to Ra < 5 nm on inch-sized wafers—directly compatible with the cleaning, lithography, and contact metallurgy processes described.
-
Customization Potential: The paper specifies a 10 mm × 10 mm die with 100 nm Au layers and 100 nm Al gates. 6CCVD supports custom metalization stacks (Au, Pt, Pd, Ti, W, Cu) with thickness control suitable for both Ohmic contacts and Schottky gates. For devices requiring smaller active areas or wafer-level processing, laser cutting and dicing services are available to deliver precision-shaped PCD pieces from larger 2-inch or 125 mm wafers.
-
Engineering Support: Reproducing the hydrogen-termination quality is critical—sheet resistance variability (5-20 kΩ/sq in literature) directly impacts FET performance. 6CCVD’s in-house PhD engineering team can advise on substrate selection, hydrogen-plasma termination parameters, and surface preparation protocols optimized for FET fabrication. Our PCD is grown via MPCVD with low impurity concentrations, providing the consistent surface quality required for high-mobility (≥170 cm2/(V·s)) channel formation.
-
Call to Action: For custom specifications, material consultation, or quotations on PCD substrates matched to hydrogen-terminated FET development, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Diamond has a great potential to be used in high-power, high-voltage and high-frequency semiconductor devices due to its wide band gap (5.5 eV), high breakdown field (> 10 MV/cm), high thermal conductivity (22 W/(cm·K)), and good carrier transport property. High-quality polycrystal diamond with large size wafers (up to several inches) is more easily obtained than the expensive monocrystal diamond plate with the size of only several mm2, and the good performance of electronic device on polycrystal diamond has been reported. So we fabricate a normally-on hydrogen-terminated polycrystal diamond field effect transistor with a 4-μm aluminum gate by using a gold mask process. The saturation drain current is 160 mA/mm, and the on-resistance is as low as 37.85 Ω ·mm. The maximum transconductance reaches 32 mS/mm, and the gate voltage range with the transconductance higher than 90% of its maximum value reaches 3 V (-2 V ≤ VGS ≤ -5 V). An Ohmic contact resistance of 5.52 Ω ·mm and a quite low square resistance of 5.71 kΩ/sq for the hydrogen-terminated diamond are extracted from the analysis of transmission line model measurement. On the basis of the analyses of the obtained results, the on-resistance of device dependent on gate voltage, and the capacitance-voltage data measured at the gate-source diode, we find that the hole sheet density under the gate reaches 1.56×1013 cm-2 at a gate voltage of -5 V, and the extracted effective mobility of the holes stays at about 170 cm2/(V·s) in the afore-mentioned gate voltage range with high transconductance. In summary, the high and broad transconductance peak and the low on-resistance are attributed to the relatively low gate-source and gate-drain series resistance, the high-density carriers in the channel, and the high-level mobility achieved over a large gate voltage range. The relevant research of finding proper dielectrics for the gate insulator and the passivation layer is under way to further improve the device performance.