Enhanced fluorescence of nitrogen vacancy diamond color center via monomer and dimer core-shell nanoresonators
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Advanced Photonics 2018 (BGPP, IPR, NP, NOMA, Sensors, Networks, SPPCom, SOF) |
| Authors | Mária Csete, András Szenes, Dávid Vass, Balázs Bánhelyi, Tibor Csendes |
| Institutions | University of Szeged |
| Citations | 1 |
Abstract
Section titled “Abstract”Fluorescence of nitrogen vacancy diamond color center was significantly enhanced via coupling to spherical and ellipsoidal, monomer and dimer, silica-silver core-shell type plasmonic nanoresonators in numerically optimized configurations.