Fourier Optical Processing Enables New Capabilities in Opto-Magnetic Imaging Using Nitrogen-Vacancy Centers in Diamond

MetadataDetails
Publication Date2018-01-01
JournalConference on Lasers and Electro-Optics
AuthorsMikael P. Backlund, Pauli Kehayias, Ronald L. Walsworth
InstitutionsCenter for Astrophysics Harvard & Smithsonian, Harvard University

Nitrogen-vacancy centers enable wide-field magnetic imaging, but ambiguities in the sample field arise in the absence of a sufficiently strong applied field. We present a solution to this issue based on Fourier optical processing.