Hybrid Diamond-Glass Optical Fibres for Magnetic Sensing
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | 26th International Conference on Optical Fiber Sensors |
| Authors | Dongbi Bai, Marco Capelli, Hoa Huynh, Heike EbendorffâHeidepriem, Scott Foster |
| Institutions | The University of Adelaide, Defence Science and Technology Group |
| Citations | 4 |
Abstract
Section titled âAbstractâWe demonstrate a new-type of magnetically sensitive optical fibre fabricated by embedding diamond lead-silicate glass. Nitrogen-vacancy centres, within the diamond particles, exhibit excellent fluorescence intensities and local magnetic field response at room temperature. DC magnetic sensitivity of the hybrid diamond-optical fibre magnetometer achieves 350. n T H z