Influence of the surface condition on the adhesion of composite materials to enamel

MetadataDetails
Publication Date2018-01-01
JournalPhysics for Economy
AuthorsMarta Szmyd, Dariusz Paliga, Andrzej Wasilewski
InstitutionsRzeszów University of Technology
Citations1

This work presents a method of measuring the maximum stress that a composite sample fixed on a tooth surface will withstand.The test was carried out for 3 different surface conditions of enamel: no processing, after treatment with a diamond drill, and after treatment with a diode laser.The force of adhesion was measured in an Instron 5960 testing machine.The results demonstrate a significant effect of the surface condition on the adhesion of the composite to the enamel.