Nanocrystalline Diamond Films Grown by Microwave Plasma Chemical Vapor Deposition and Its Biocompatible Property
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Advances in Materials Physics and Chemistry |
| Authors | Jihan Yang, Yongping Zhang |
| Institutions | Southwest University |
| Citations | 6 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Material Focus: Comprehensive review of Nanocrystalline Diamond (NCD) and Ultra-Nanocrystalline Diamond (UNCD) films deposited via Microwave Plasma Chemical Vapor Deposition (MPCVD), targeting biomedical implant applications.
- Key Structural Achievement: Grain size control between 2 nm to 100 nm, with UNCD specifically defined as 2-10 nm grains containing sp2-C grain boundaries for sustained surface smoothness independent of film thickness.
- Doping Capabilities: Successful p-type and n-type semiconductor NCD fabrication via boron and nitrogen doping respectively, achieving resistivities down to 10-2 Ω·cm for boron-doped films.
- Mechanical Performance: Hardness range of 35-75 GPa with friction coefficients as low as 0.02 (an order of magnitude lower than microcrystalline diamond), accompanied by surface roughness < 30 nm on optimized substrates.
- Biocompatibility Validation: Demonstrated cell adhesion, proliferation, and differentiation success on NCD/UNCD surfaces across neural, osteoblast, fibroblast, and embryonic stem cell lines, with hydrogen-termination yielding hydrophobic/conductive surfaces and oxygen-termination yielding hydrophilic/resistive surfaces.
- Primary Deposition Advantage: MPCVD achieves high growth rates up to 9.6 µm/h at substrate temperatures of 300-1000°C, avoiding filament contamination inherent to Hot Filament CVD while enabling electrode-free high-purity plasma generation.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| NCD Grain Size | 10-100 | nm | Standard nanocrystalline diamond regime |
| UNCD Grain Size | 2-10 | nm | Ultra-nanocrystalline regime with sp2 boundaries |
| Microcrystalline Grain Size | >10,000 | nm | Reference comparison |
| NCD Hardness | 35-75 | GPa | Comparable to natural diamond |
| Microcrystalline Hardness | 100 | GPa | Reference comparison |
| NCD Friction Coefficient | 0.02 | — | Coefficient of friction |
| NCD Young’s Modulus | 1100 | GPa | Elastic modulus |
| NCD Surface Roughness (min) | < 30 | nm | With optimized TiO2 interlayer |
| NCD Roughness on Mo Seed | 20.8 | nm | Metallic seed layer comparison |
| NCD Roughness on Ti Seed | 23.7 | nm | Metallic seed layer comparison |
| NCD Roughness on W Seed | 19.4 | nm | Metallic seed layer comparison |
| NCD Roughness on Glass | ~28 | nm | Alcaide et al. fibroblast study |
| NCD Roughness on Ti | ~110 | nm | Alcaide et al. fibroblast study |
| Boron-Doped Resistivity | 10-2 | Ω·cm | Minimum achievable conductivity |
| Field Emission Onset Field | 0.36 | V/µm | Boron-doped NCD |
| Turn-On Field (N-doped UNCD) | 3.4 | V·µm-1 | At 830°C deposition |
| Peak Current Density | 8.0 | mA·µm-2 | N-doped UNCD |
| Growth Rate (CH4/H2/N2/O2) | 2.6 | µm/h | High microwave power regime |
| Growth Rate (In-Liquid Plasma) | 8.5 | µm/h | Novel Harada et al. method |
| Growth Rate (3 kW MPCVD, N2) | 5.4-9.6 | nm/h | Nitrogen incorporation regime |
| Band Gap (High Purity Diamond) | 5.5 | eV | Wide-bandgap semiconductor |
| sp3 Content (Low-Temp MPCVD) | 84.77 | % | Quality indicator |
| Argon Plasma Fraction (UNCD) | 95-99 | % | Gas precursor composition |
| Electron Density (MPCVD Plasma) | 1011 | cm-3 | High-density plasma regime |
| Deposition Pressure (ECR regime) | 1-2.7 | mTorr | Low-pressure operation |
| Standard Deposition Pressure | 28 | Torr | Typical MPCVD operation |
| Substrate Temperature Range | 300-1000 | °C | MPCVD operational window |
| Microwave Power (Standard) | 550-1200 | W | Typical operating range |
| Microwave Power (High-Rate) | 3000-4000 | W | High-growth-rate regime |
Key Methodologies
Section titled “Key Methodologies”-
Substrate Preparation and Seeding
- Select substrate material (Si, Si3N4, Ti, glass, or metallic seed layers: Mo, Ti, W).
- Apply surface pre-treatments to enhance nucleation density.
- Optionally deposit TiO2 interlayer via magnetron sputtering for roughness control.
-
Gas Precursor Selection
- Standard NCD: Use CH4/H2 mixtures with optional N2 or O2 addition.
- UNCD: Employ Ar-rich, H2-poor environment (Ar: 95-99%, H2: 1-4%, CH4: 1-2%).
- p-type Doping: Introduce boron-containing precursors during CVD growth.
- n-type Doping: Use CH4/N2, CH4/H2/N2, or Ar/CH4/N2 gas mixtures.
-
Plasma Generation and Deposition
- Ignite microwave plasma without internal electrodes to maintain film purity.
- Maintain substrate temperature within 300-1000°C range (typically 460-830°C).
- Control chamber pressure according to regime: 1-2.7 mTorr (ECR) to 28 Torr (standard MPCVD).
-
Process Optimization Parameters
- Apply microwave power between 550 W (standard) and 4000 W (high-rate growth).
- Apply negative substrate bias (e.g., -250 V) for bias-enhanced nucleation and growth.
- Monitor CH4 flow rate (e.g., 1 sccm) with carrier gas ratio control.
-
Post-Deposition Characterization
- Confirm sp3 content via XPS (target > 84%).
- Analyze D-band, G-band, and diamond peaks via Raman spectroscopy.
- Quantify surface roughness via SEM and profilometry.
- Validate biocompatibility through cell adhesion and proliferation assays.
-
Surface Termination Engineering
- Hydrogen-terminate for hydrophobic/conductive surfaces.
- Oxygen-terminate for hydrophilic/resistive surfaces.
- Graft functional groups (H, O, hydroxyl, carboxyl) for tailored bio-interfaces.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials
- Optical/Mechanical Grade PCD directly corresponds to the NCD/UNCD thin films discussed in this review, particularly for biomedical implant coatings requiring low friction (< 0.02) and high hardness (35-75 GPa) regimes.
- Heavy Boron-Doped PCD (BDD) is the commercial analog to the p-type doped NCD achieving 10-2 Ω·cm resistivity, suitable for retinal implant electrodes, biosensors, and cell-based sensing platforms.
- Optical Grade SCD is recommended for applications requiring the highest electron mobility and bandgap purity (5.5 eV), such as photonic crystal microcavities and UV Schottky contacts referenced in the paper.
- Custom NCD/UNCD Films with grain sizes spanning 10-100 nm are produced via our MPCVD reactor fleet, matching the deposition parameters characterized in this study.
-
Customization Potential
- Wafer Dimensions: Plates and wafers up to 125 mm (PCD) enable large-area biomedical coatings and AFM cantilever arrays; thicknesses from 0.1 µm to 500 µm satisfy both thin-film encapsulation (UNCD on retinal microchips) and bulk substrate requirements.
- Metallization Stack Engineering: The paper highlights Mo, Ti, W seed layers and TiO2 interlayers. 6CCVD offers in-house metallization with Au, Pt, Pd, Ti, W, and Cu, allowing full customization of buffer/seed layer architectures for optimized nucleation and adhesion.
- Laser Cutting Services: Custom geometries for implant components, heart valve rings, and dental implant form factors are achievable through our precision laser cutting capabilities.
- Polishing Specifications: For applications demanding optical-grade smoothness, we deliver Ra < 1 nm on SCD and < 5 nm on inch-size PCD, critical for ophthalmological and neural interface applications where surface roughness directly influences protein adsorption and cell adhesion.
-
Engineering Support
- Our in-house PhD engineering team provides direct consultation on material selection for biomedical implant projects, including diamond-coated hip prostheses, femoral heads, artificial heart valves, cochlear implants, and dental implants.
- We assist with doping concentration optimization for boron (p-type) and nitrogen (n-type) semiconductor diamond applications, including field emission devices and electrochemical biosensors.
- Our team can replicate and extend the MPCVD parameters detailed in this review—substrate temperatures of 300-1000°C, microwave power scaling to 4 kW, and custom gas precursor recipes including CH4/H2/N2/O2 and Ar-rich UNCD formulations.
-
Call to Action
- For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Due to its unique properties such as high hardness, light transmittance, thermal conductance, chemical stability and corrosion resistance, diamond has drawn tremendous attention in last two decades. These specific properties made diamond film a promising material for cutting tools, microwave windows, heat sinks for electronic devices and diamond electrodes. However, the diamond film with grain sizes at microscale usually exhibits high surface roughness and hinders its applications in the microelectro mechanical system (MEMS) and biological field because it is difficult to be polished by mechanical and chemical methods. With the development of the chemical vapor deposition, the nanocrystalline diamond (NCD) film has been fabricated and found new applications. The grain size of NCD film is in the range of 10 to 100 nm, which inherits the properties of the diamond and possesses the unique properties of the nanoscale materials, and the morphology of the NCD film is granular or needle-like structure. The microwave plasma chemical vapor deposition (MPCVD) has been regarded as the most promising method to deposit NCD film at low temperature. Compared to the hot filament CVD, MPCVD can grow high quality NCD film avoiding of the contamination from the filament materials. The MPCVD technique has high plasma density to activate carbonaceous compound and grow NCD film in high growth rate and low substrate temperature. The unique properties of NCD film, such as the superior electrical, mechanical and biological properties facilitate their application in various fields. The biological application, especially as a biocompatible coating, mainly includes the joint replacement implants and protective coatings and the ophthalmological prosthesis.