Resonant phonon scattering in semiconductors
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Journal | Journal of Materials Chemistry C |
| Authors | Bonny Dongre, JesĆŗs Carrete, Ankita Katre, Natalio Mingo, Georg K. H. Madsen |
| Institutions | CEA LITEN, CEA Grenoble |
| Citations | 23 |
Abstract
Section titled āAbstractāThe origins of the dramatic effect of some dopants on the thermal conductivity of semiconductors are studied. By analyzing the cases of B-doped 3C-SiC, B-doped diamond, N-doped diamond and a simple linear chain model, small symmetry breaking structural distortions and a high density of states are identified as the key ingredients in resonant phonon scattering.