In this paper, the acoustic mismatch model and the differential effective medium scheme were applied to predict the influence of different interfacial coatings (Si and SiC) on the interfacial thermal conductivity and thermal conductivity of the Diamond/Al composites, respectively. With the increase of the thickness of interfacial coatings, the interfacial thermal conductivity and of the thermal conductivity of Diamond/Al composites decreased. In order to obtain ideal thermal conductivity of Diamond/Al composites, the thickness of the coating should be controlled below 1 μ m. When the volume fraction of diamond was 60% and the average particle size was 100 μ m, the interfacial thermal conductivity of Si and SiC coated Diamond/Al composites were in the range of 1.77Ɨ10 7 ∼1.1Ɨ10 8 W/(m 2 Ā· K) and 2.44Ɨ10 7 ∼1.29Ɨ10 8 W/(m 2 Ā· K), respectively; the thermal conductivity of Si and SiC coated Diamond/Al composites were in the range of 541.58∼764.15 W/(mĀ· K) and 594.45∼777.3 W/(mĀ· K), respectively. The thermal conductivity of Si and SiC coated Diamond/Al composites increased with the volume fraction and average particle size of Diamond, and the thermal conductivity of SiC coated Diamond/Al composites was higher than that of Si coated composites. SiC interface coating was proposed to be the most promising candidates to improve the thermal performance of Diamond/Al composites.

  1. 2014 - Emerging challenges and materials for thermal management of electronics [Crossref]
  2. 2017 - Thermal boundary conductance of a new generation of high thermal conductivity metal matrix composites: A review
  3. 2006 - Selective interfacial bonding in Al(Si)-diamond composites and its effect on thermal conductivity [Crossref]
  4. 2006 - Effect of diamond crystallographic orientation on dissolution and carbide formation in contact with liquid aluminium [Crossref]
  5. 2016 - Nucleation and growth mechanisms of interfacial Al4C3 in Al/diamond composites [Crossref]
  6. 2014 - Enhanced thermal conductivity and stability of diamond/aluminum composite by introduction of carbide interface layer [Crossref]
  7. 2016 - Effect of (0-40) wt.% Si addition to Al on the thermal conductivity and thermal expansion of diamond/Al composites by pressure infiltration [Crossref]
  8. 2011 - Microstructure and thermal properties of diamond-Al composite fabricated by pressureless metal infiltration
  9. 2012 - Effect of copper content on the thermal conductivity and thermal expansion of Al-Cu/diamond composites [Crossref]
  10. 2010 - Microstructure and thermal properties of diamond/aluminum composites with TiC coating on diamond particles [Crossref]