Thermal characterization of polycrystalline diamond using infrared thermal imaging measurement
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-01-01 |
| Authors | Beng Kang Tay, Qinyu Kong, Laurence Bodelot, Bérengère Lebental, D.S. Misra |
| Institutions | Centre National de la Recherche Scientifique, Laboratoire de Physique des Interfaces et des Couches Minces |
Abstract
Section titled “Abstract”Thermal characterization of polycrystalline diamond based on an infrared thermal imaging technique is proposed. The temperature mapping of polycrystalline diamond under a metal wire heating are recorded using a $15~\mu \text{m}$-resolution infrared thermal imaging system. The thermal conductivity of the polycrystalline diamond is derived from the temperature profile using numerical fitting with a 3D heat diffusion model. The thermal conductivity of the polycrystalline diamond is also determined using a $3\omega$ technique. The agreement between the thermal conductivities measured using these two techniques is within 15%.