Electrochemical Behavior of Boron-doped Synthetic Diamond Compacts - A New Electrode Material
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-03-28 |
| Journal | 2018-Sustainable Industrial Processing Summit |
| Authors | Yu. V. Pleskov, M. D. Šrotova, Eugeniy Ekimov |
Abstract
Section titled āAbstractāTraditional thin-film synthetic diamond electrodes produced by chemical-vapor deposition (CVD, see [1, 2]) are remarkable for their wide potential window and low background current in supporting electrolytes and good reproducibility. However, they are not free of disadvantages, particularly from the film exfoliation from substrate, thru-holes, etc. In this work we presented a new electrode material, heavily boron-doped diamond compacts whose electrochemical properties are studied for the first time. Cylinder-shaped polycrystalline samples, 3.5-4 mm in diameter and 2.5 mm in height, were prepared by thermobaric processing of graphite-boron carbide mixtures at the pressure of 8-9 GPa and temperature of ~2500 K [3]. Their diamond nature, in particular, the absence of graphite, was confirmed by Raman spectroscopy and XRD technique. Their electrode behavior is studied by using cyclic voltammetry and electrochemical impedance spectroscopy. The compacts are shown to be superior to conventional thin-film CVD-diamond electrodes in their electrode characteristics. In particular, they have wide potential window, low background current in indifferent electrolytes (KCl, K2SO4), and good reproducibility. Moreover, their extremely high doping level makes them more electroactive, as can be seen by the current of Cl2 anodic evolution from KCl solutions (figure), some organics electrooxidation, etc. [4].
Thus, the diamond compacts are well comparable to the CVD-diamond electrodes. At the same time, they are free of some drawbacks inherent in the latter. Moreover, their concentrated form can be advantageous in the designing of electrochemical devices. One might think that they can successfully be used, e.g., as electrodes in electrosynthesis, electroanalysis, water treatment, etc. [5].
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None