Search for a new member of parabolic-like spin-gapless semiconductors - The case of diamond-like quaternary compound CuMn2InSe4
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-06-18 |
| Journal | Results in Physics |
| Authors | Yilin Han, R. Khenata, Tingzhou Li, Liying Wang, Xiaotian Wang |
| Institutions | Southwest University, Tianjin University |
| Citations | 26 |
Abstract
Section titled āAbstractāSpin-gapless semiconductors (SGSs) can be viewed as a potential upcoming candidate for spintronic applications, which bridge semiconductors and half-metallic materials (HMMs). In general, one of the spin directions is semiconducting while the other has a zero band gap. Until now, the concrete theory of SGS systems has not been developed and proved. There are limited investigations on the design of the theory of SGS systems and the availability of experimental data is very few. In this paper, a new possible candidate for parabolic-type SGS has been proposed in diamond-like quaternary compound, CuMn2InS4. Moreover, this compound has already been prepared and we hope the magneto-transport properties can be measured at low temperature to confirm its SGS behavior from experiment. Keywords: Spin-gapless semiconductors, Electronic structure, Magnetism
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2015 - First-principles prediction of the structural, elastic, thermodynamic, electronic and optical properties of Li4Sr3Ge2N6 quaternary nitride [Crossref]
- 2003 - Calculation of structural, optical and electronic properties of ZnS, ZnSe, MgS, MgSe and their quaternary alloy Mg1āxZnxSySe1āy [Crossref]
- 2015 - Structural, elastic, electronic and optical properties of the quaternary nitridogallate LiCaGaN2: first-principles study [Crossref]
- 2016 - Ultrasonic effect on optical, structural, topographical and morphological studies of Cu2CdSnS4 quaternary alloy nanostructures [Crossref]
- 2018 - First-principle calculations of structural, electronic and magnetic investigations of Mn2RuGe1-xSnx quaternary Heusler alloys [Crossref]
- 2017 - A needle-like Cu2CdSnS4 alloy nanostructure-based integrated electrochemical biosensor for detecting the DNA of Dengue serotype 2 [Crossref]
- 2018 - Ab initio investigation of the structural, electronic and optical properties of the Li2In2XY6 (X = Si, Ge; Y = S, Se) compounds [Crossref]
- 2014 - Synthesis and crystal structure of the quaternary compound AgFe2GaTe4 [Crossref]
- 2003 - New materials for spintronics [Crossref]
- 2010 - Fabrication of 7.2% efficient CZTSSe solar cells using CZTS nanocrystals [Crossref]