Skip to content

DISCRETE STEPS OF DIAMOND-GRAPHITE PHASE TRANSITION AT ANNEALING OF NANODIAMONDS IN WIDE TEMPERATURE RANGE

MetadataDetails
Publication Date2018-07-17
JournalIZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENIY KHIMIYA KHIMICHESKAYA TEKHNOLOGIYA
AuthorsNikolay E. Kornienko, А. Н. Кириченко
Citations2
AnalysisFull AI Review Included
  • Investigation Focus: Detailed Raman spectroscopy (514.5 nm laser) analysis of nanodiamonds (ND) subjected to high-temperature vacuum annealing to map the diamond-to-onion-like carbon (OLC) phase transition.
  • Thermal Range Tested: Isothermal annealing conducted across a broad range of 900 °C to 2000 °C, with specific data points at 940, 980, 1000, 1200, 1300, 1500, 1800, and 2000 °C.
  • Key Discovery: The phase transition does not occur at a single thermodynamic threshold but proceeds via discrete steps, characterized by specific temperature maxima (940-1200 °C and 1500-2000 °C) in spectral intensity, FWHM, and frequency shifts.
  • Spectral Decomposition: Standard D and G Raman bands (indicative of sp2/sp3 carbon ratios) were successfully decomposed into individual spectral components: D, G, D(k), D(k’), and G(k’), correlating to specific Brillouin Zone states (center vs. boundary).
  • Anomalous Behavior: Extreme intermediate states were observed, evidenced by a broadband electronic background peaking near 940 °C and an anomalous positive anharmonic shift (Δν ≈ 25 cm-1) in the 2D overtone at extreme temperatures.
  • Process Environment: Annealing performed under high vacuum conditions (10-4 Torr) for a 1-hour dwell time, simulating extreme thermal stress on the sp3 crystal lattice.
  • Practical Implication: The research confirms the existence of intermediate carbon states with altered electronic and vibrational properties, which has direct implications for engineering thermal stability in carbon-based devices.
ParameterValueUnitContext & Observation
Laser Excitation Wavelength514.5nmRaman scattering spectrometer (TRIAX 552, Jobin Yvon)
Laser Power at Sample~1mWFocused spot size of 2 µm
Annealing Vacuum Pressure10-4TorrBase pressure for thermal processing
Annealing Dwell Time1hourIsothermal hold at target temperature
Annealing Temperature Range900 - 2000°CLower bound of observable phase change to upper limit
Key Data Point Temperatures940, 980, 1000, 1200, 1300, 1500, 1800, 2000°CSpecific thermal setpoints for Raman sampling
D Band Frequency (Graphite-like)~1326 - 1346cm-1Shift observed between 25 °C and 1800 °C
G Band Frequency (Graphite-like)~1542 - 1589cm-1Narrowed to 65 cm-1 FWHM at 1800 °C
D(k) Component Frequency~1140 - 1160cm-1Boundary of Brillouin Zone state (post-anneal)
Local Electronic Band (EB) FWHM~200cm-1Observed in initial ND; signifies hybrid vibronic state
Anomalous Anharmonic Shift (2D)~25cm-1Positive shift at high-temperature transition phase
  1. Sample Preparation: Acquire agglomerated nanodiamond (ND) powder and subject to high-vacuum thermal annealing (10-4 Torr) for 1 hour at target temperatures.
  2. Annealing Protocol: Execute a stepped thermal profile across the 900 °C to 2000 °C envelope, isolating specific structural transitions at 940, 980, 1000, 1200, 1300, 1500, 1800, and 2000 °C.
  3. Raman Spectroscopy: Analyze the annealed samples using a 514.5 nm laser at low power (~1 mW) with a 2 µm spot size to avoid thermal damage to the nanostructures.
  4. Spatial Averaging: Record spectra at multiple, spatially distinct locations on each agglomerated sample and average the data to account for material heterogeneity.
  5. Spectral Processing: Apply optimal smoothing algorithms and subtract the broadband electronic background to isolate the vibrational D and G bands.
  6. Component Decomposition: Perform numerical deconvolution of the D and G bands into individual Lorentzian spectral components (D, G, D(k), D(k’), G(k’)) to map distinct Brillouin Zone phonon states.
  7. Kinematic Analysis: Track the temperature dependence (T) of peak intensity (Imax), frequency shift (ν), and full width at half maximum (δν) for each spectral component to identify discrete phase transition stages.

The research detailed in this paper relies on the precise characterization of the sp3 to sp2 transition under extreme thermal loads. Replicating or building upon this thermal stability testing requires CVD diamond materials with verified crystalline integrity. Below is how our capabilities align with these experimental demands:

  • Applicable Materials:

    • For studies focusing on the bulk phase transition of isolated crystals, our Optical Grade Single Crystal Diamond (SCD) is ideal due to its ultra-low defect density and known thermal baselines.
    • For studies simulating the boundaries and grain structures of the nanodiamond agglomerates analyzed here, our High-Purity Polycrystalline Diamond (PCD) provides a robust, macroscopically testable analog.
    • If electronic or electrochemical properties are being tested in these intermediate transition states, our Boron-Doped Diamond (BDD) offers tunable conductivity to complement the study’s “local electronic bands.”
  • Customization Potential:

    • The paper utilizes agglomerated ND powder, but extending this research to device fabrication (e.g., MEMS or thermal management) requires specific geometries. 6CCVD provides custom PCD plates and wafers up to 125mm, allowing researchers to scale up bulk thermal transition tests.
    • We offer internal metalization capabilities (Au, Pt, Pd, Ti, W, Cu). Should this phase transition research require creating in-situ heating elements or electrode interfaces for Raman testing, we can provide custom metalized SCD/PCD substrates.
    • Precision laser cutting and polishing services (achieving Ra < 1nm for SCD and < 5nm for inch-size PCD) are available to prepare the exact surface roughness required for accurate spectroscopic baseline measurements.
  • Engineering Support:

    • Understanding the discrete steps of the diamond-graphite phase transition is critical for designing devices intended for high-temperature or high-power environments (e.g., thermal sinks, quantum sensors, or extreme UV optics).
    • 6CCVD’s in-house PhD engineering team can assist with material selection for your specific high-temperature Raman spectroscopy or extreme environment projects, helping you choose the correct dopant levels, crystal orientation, and thickness (from 0.1µm thin films to 10mm substrates) to maximize your experimental yield.
  • Call to Action: For custom specifications, specialized metalization, or material consultation regarding your high-temperature diamond research, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

We present the short review of the works on a problem of phase transitions (PT) which are distributed in the temperature range ΔТ of PT. Experimental studies of Raman spectra (laser wavelength 514.5 nm) of nanodiamonds after annealing at 900-2000 °C and their detailed numerical analysis with decomposition of the allocated oscillatory D and G bands on the compound spectral components D and G, D (k) and G (k’) relating to various states of Brillouin’s zones were conducted. Detection of temperature maxima of intensities, frequencies and full width at half maximum (FWHM) of individual Raman components as well as intensity of a background defines discrete steps of PT of diamond - onion-shaped carbon in temperature ranges of 940-1200 °C and 1500-2000 °C.