CRYSTALLOGRAPHIC ORIENTATION INFLUENCE ON SECONDARY ELECTRON EMISSION COEFFICIENT OF A SINGLE CRYSTAL OF SYNTHETIC DIAMOND
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-07-17 |
| Journal | IZVESTIYA VYSSHIKH UCHEBNYKH ZAVEDENIY KHIMIYA KHIMICHESKAYA TEKHNOLOGIYA |
| Authors | Vladimir Yu. Sadovoy, В. Д. Бланк, S.A. Terentiev, Dmitriy V. Teteruk, S. Yu. Troschiev |
| Citations | 1 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Objective: Quantify how crystallographic orientation governs the Secondary Electron Emission (SEE) coefficient in synthetic single-crystal diamond (Type IIb) for next-generation microchannel plate (MCP) and detector applications.
- Material: Boron-doped (Type IIb) single-crystal diamond grown via Temperature Gradient Method (TGM), with boron concentration ~1017 cm-3 and thickness ≥ 200 µm.
- Critical Finding — Orientation Dependence: The cubic (100) sector and the intergrowth regions deliver SEE coefficients 4-6× higher than the octahedral (111) sector, directly correlating with lower impurity/defect density and superior crystalline quality.
- Record Performance: SEE coefficient of 64.41 measured in intergrowth regions at 30 keV primary beam energy — an order of magnitude higher than conventional emitters (literature reference: 30-50), enabling diamond-based MCP fabrication.
- Anomalous Behavior: Non-standard monotonic increase of SEE coefficient across the 7-30 keV range for all orientations; mechanism remains unexplained and flagged for further structural/surface investigation.
- Surface Engineering: Hydrogen termination via CVD plasma processing at 1200°C for 30 minutes establishes Negative Electron Affinity (NEA, ~ -1.3 eV), critical for low-energy electron emission without energy loss.
- Application Impact: Results open pathways for diamond-based X-ray optics, particle detectors, and a new branch of microelectronics replacing conventional functional elements.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Diamond Type | IIb (boron-doped, semiconducting) | — | Selected for microelectronic applicability |
| Boron Concentration | ~1017 | cm-3 | Low doping regime |
| Growth Method | Temperature Gradient Method (TGM) | — | HPHT synthesis route |
| Sample Thickness | ≥ 200 | µm | Exceeds primary beam interaction depth |
| Electron Affinity (H-terminated) | ~ -1.3 | eV | Nemanich et al.; Cui et al. references |
| SEE Coefficient — (100), 7 keV | 8.18 | — | Cubic sector |
| SEE Coefficient — (100), 10 keV | 10.13 | — | Cubic sector |
| SEE Coefficient — (100), 30 keV | 49.78 | — | Cubic sector |
| SEE Coefficient — (111), 7 keV | 2.54 (avg.) | — | Octahedral sector |
| SEE Coefficient — (111), 10 keV | 2.75 | — | Octahedral sector |
| SEE Coefficient — (111), 30 keV | 10.03 | — | Octahedral sector |
| SEE Coefficient — Intergrowth, 7 keV | 10.10 | — | Intergrowth region |
| SEE Coefficient — Intergrowth, 10 keV | 13.56 | — | Intergrowth region |
| SEE Coefficient — Intergrowth, 30 keV | 64.41 | — | Intergrowth region (record) |
| SEE Enhancement Ratio | 4-6× | — | (100)/Intergrowth vs. (111) |
| Primary Beam Energy Range | 7-30 | keV | SEM investigation range |
| Plasma Power (H-termination) | 3.25 | kW | CVD reactor |
| Annealing Temperature | 1200 | °C | H-termination process |
| Annealing Duration | 30 | min | Hold time at target temperature |
Key Methodologies
Section titled “Key Methodologies”- Sample Selection: Type IIb single-crystal diamond grown by Temperature Gradient Method with low boron concentration (~1017 cm-3).
- Mechanical Preparation: Surface polished to optical quality, then sequentially cleaned in acetone (ultrasonic bath) followed by isopropanol.
- Hydrogen Termination Protocol:
- Slow ramp to 1200°C inside CVD chamber under hydrogen plasma.
- 3.25 kW plasma power maintained for 30 minutes.
- Slow cool-down to prevent thermal shock cracking.
- Characterization Techniques:
- UV fluorescence imaging — identified N3 nitrogen-vacancy centers in “blue” sectors vs. impurity-free “dark” sectors.
- True Secondary Electron (TSE) detector imaging in SEM — mapped SEE intensity distribution across growth sectors.
- Quantitative SEE Measurement: Primary electron beam energies swept from 7 keV to 30 keV; SEE coefficient recorded for six measurement points spanning (100), (111), and intergrowth regions.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”| Research Requirement | 6CCVD Capability |
|---|---|
| High-purity (100)-oriented Type IIb diamond | Optical-Grade Single Crystal Diamond (SCD) with controlled crystallographic orientation |
| Boron doping ~1017 cm-3 | Light/Medium Boron-Doped Diamond (BDD) — tunable doping profiles |
| TGM-grown single crystal ≥ 200 µm | SCD thickness range 0.1 µm - 500 µm; substrate-grade options up to 10 mm |
| Hydrogen-terminated surface (NEA) | In-house MPCVD plasma processing for H-termination protocols |
| Custom wafer dimensions | Plates/wafers up to 125 mm (PCD) with custom laser cutting |
| Surface finish for SEE measurements | SCD polishing to Ra < 1 nm |
Applicable Materials
Section titled “Applicable Materials”- Optical-Grade SCD (100 orientation): Directly matches the optimal cubic sector identified in this work for maximum SEE coefficient and largest effective device area.
- Light Boron-Doped BDD (Type IIb equivalent): For replicating semiconductor-grade single crystal behavior with controlled carrier concentration.
- High-Purity PCD: An alternative if larger active areas are required beyond single-crystal sector limitations.
Customization Potential
Section titled “Customization Potential”- Custom Metalization: Although this paper focuses on bare diamond surface physics, downstream MCP fabrication typically requires patterned electrodes. 6CCVD offers in-house metalization with Au, Pt, Pd, Ti, W, and Cu — enabling Ti/Pt/Au or Cr/Au multilayer stacks for contact formation.
- Laser Cutting & Shaping: Intergrowth regions and specific sector orientations can be precision-machined to your device geometry.
- Surface Engineering: Tailored H-termination, oxygen termination, or alkali-halide coating protocols per Mearini et al. reference for enhanced SEE stability.
Engineering Support
Section titled “Engineering Support”6CCVD’s in-house PhD engineering team can assist with:
- Material selection guidance for microchannel plate (MCP) development, X-ray optics, and secondary electron emission devices.
- Doping concentration tuning to optimize the trade-off between conductivity and SEE yield.
- Surface preparation recipe development for Negative Electron Affinity (NEA) applications.
Call to Action: For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Dependence of secondary electron emission coefficient on the chosen crystallographic orientation for a synthetic single crystal diamond of type IIb, grown up by method of a temperature gradient, was investigated. The type IIb of single crystal diamond was chosen because of wide applicability in different areas of microelectronics and the semiconductor properties. Quantitative measurements of secondary electron emission coefficients with energy of primary beam about 7 keV and above for various crystallographic orientations was carried out: the highest coefficient of secondary electronic emission are recorded for the direction (100), cubic sector, and also in intergrowth area that is confirmed by a picture of distribution of the luminescence intensity for various sectors of a single crystal received by means of true secondary electrons detector of scanning electron microscope. The results for (100) area are outstanding: 8.18 at primary beam energy of 7 keV, 10.13 at 10 keV, 49.78 at 30 keV. The results for intergrowth area are similar: 10.10 at primary beam energy of 7 keV, 13.56 at 10 keV, 64.41 at 30 keV. The crystallographic directions (111) have shown secondary electron emission coefficient 4-6 times lower in comparison with (100) and intergrowth area: 2.54 on the average at primary beam energy of 7 keV, 2.75 at 10 keV, 10.03 at 30 keV. The non-standard behavior of secondary electron emission coefficient at the high energy primary beam for all orientations of single crystal diamond is shown: increase in secondary electron emission coefficient with increase in energy of primary beam. At the moment the reason of such behavior is not clear up to the end and since this fact causes a great interest of researchers, considerably expands applicability of the existing devices and detectors due to replacement of a functional element on diamond one, and also opens big opportunities for formation of new field of microelectronics, this facts demand further in-depth study by means of various methods of the structural and surface analysis.