Skip to content

Cover Feature - Facile Deposition of Cu−SnOx Hybrid Nanostructures on Lightly Boron‐Doped Diamond Electrodes for CO2 Reduction (ChemElectroChem 18/2018)

MetadataDetails
Publication Date2018-08-03
JournalChemElectroChem
AuthorsNitish Roy, Norihiro Suzuki, Yukihiro Nakabayashi, Yuiri Hirano, Hiroshi Ikari
InstitutionsTokyo University of Science

The Cover Feature illustrates hybrid nanoparticles of Cu−SnOx on a lightly boron-doped diamond substrate by using simple potentiodynamic electrodeposition to enhance selective CO2 reduction to CO with a suppression of H2 production. More information can be found in the Article by N. Roy et al. on page 2542 in Issue 18, 2018 (DOI: 10.1002/celc.201800460).