Probing a Spin Transfer Controlled Magnetic Nanowire with a Single Nitrogen-Vacancy Spin in Bulk Diamond

MetadataDetails
Publication Date2018-09-13
JournalNano Letters
AuthorsAdrian Solyom, Zackary Flansberry, Märta A. Tschudin, Nathaniel Leitao, Michel Pioro-Ladrière
InstitutionsMcGill University, Institut quantique
Citations18
AnalysisFull AI Review Included

Probing Spin Transfer Controlled Magnetic Nanowire with NV-Diamond Quantum Sensing

Section titled “Probing Spin Transfer Controlled Magnetic Nanowire with NV-Diamond Quantum Sensing”
  • Core Achievement: Unambiguous, phase-locked ferromagnetic resonance (FMR) detection of spin-transfer-torque (STT) driven parametric magnetic oscillations in an 8 µm × 417 nm Permalloy (Ni81Fe19)/Pt bilayer nanowire.
  • NV-Diamond Quantum Sensing: Single nitrogen-vacancy (NV) centers implanted ~60 nm below the diamond surface act as atomic-scale magnetometers to detect stray fields and local magnetic noise from a proximal nanowire.
  • NV-Driven Magnetic Oscillations: The stray field oscillations from the nanowire alone drive NV spin transitions, removing ambiguity from traditional transport measurements and offering a novel spin-qubit control modality.
  • Spin Transfer Cooling (STC): Application of STT reduces stray-field magnetic noise by orders of magnitude, consistent with magnetic cooling from 300 K down to ~150 K—a 2× improvement over Brillouin light scattering (BLS) on analogous structures.
  • Multi-Magnon Suppression: Observed precession angles up to ~55° without Suhl-like instabilities, attributed to suppressed multi-magnon scattering in the confined nanowire geometry.
  • Fabrication Demands: Requires ultra-smooth electronic-grade single-crystal diamond (Ra < 0.2 nm) with shallow, high-fidelity NV ensembles, plus patterned Ti/Pt/Au contact metallization.

ParameterValueUnitContext
Diamond SubstrateElectronic grade CVD SCD—Host for NV sensing layer
NV Implantation Depth60 ± 15 nmnmReduced from 75 nm via post-anneal plasma etch
Implantation Species15N+—60 keV energy, Innovion Corp.
Surface Roughness (Pre-deposition)~0.2 nm RMS (micron-scale)nmAchieved via Ar/Cl2 etching
Surface Roughness (Small-scale)~0.05 nm RMSnmSub-micron measurement
Nanowire MaterialPermalloy (Ni81Fe19) / Pt bilayer—Multilayer spin Hall heterostructure
Nanowire Dimensions8 µm × 417 nm × 20 nm (10+10)µm / nmLength × Width × Thickness
Active Region Length5.2 µmµmExposed between Ti/Au contacts
Macroscopic LeadsTi (10 nm) / Au (50 nm / 70 nm)nmE-beam / photolithography
Saturation Magnetization (Py)~525 (µ₀Ms)mTFitted from Kittel model
In-plane Anisotropy Field (µ₀Hyx)7.57 ± 0.08mTMacrospin model fit
Out-of-plane Anisotropy (µ₀Hzx)517 ± 4mTMacrospin model fit
Static Field Range10-40mTApplied along NV axis (35° from y)
FMR Frequency Range~1.6-2.7GHzField-dependent
Bias Current (I0) Range-4.08 to +4.9mASpin transfer control
RF Current Amplitude~0.95-1.15mAParametric drive
Parametric Resonance Peak~120µVAt I0 = 4.08 mA
Maximum Precession Angle~55-60°From AMR & stray-field reduction
Maximum Linewidth (Δν)~600MHzFundamental mode
Magnetic Cooling Estimate~300 K → ~150 KKST-damped noise floor
Joule Heating Bound≲5KOver full bias range
Wire Resistance237.3 ± 0.3ΩDifferential measurement
Temperature Coefficient5.3085 × 10⁻⁴mA⁻²Fractional change
Spin Hall Efficiency (ηθ_SH)0.055—Literature value
g-factor (Py)2.09—10 nm film thickness

  1. Diamond Surface Preparation: Electronic-grade CVD diamond polished via Ar/Cl₂ inductively-coupled plasma etching to <0.2 nm RMS roughness.
  2. NV Center Creation: 15N+ ion implantation (60 keV) followed by high-temperature annealing; depth reduced to 60 ± 15 nm via subsequent Ar/O₂ plasma etch (20 mTorr, 35 sccm Ar, 10 sccm O₂, 108 W RF, 45 s).
  3. Surface Termination: Boiling 1:1:1 nitric/perchloric/sulfuric acid at 200°C for 1 hour to oxygen-terminate the surface.
  4. Nanowire Fabrication: E-beam lithography, sputtering, and liftoff of Py(10 nm)/Pt(10 nm) bilayer (evaporation recommended for improved liftoff yield).
  5. Contact Metallization: Ti(10 nm)/Au(50 nm) macroscopic leads and 10 µm-wide microwave stripline via photolithography.
  6. NV Optical Pumping: 532 nm laser excitation with PL collection >594 nm; ESR spectroscopy identifies NV orientations.
  7. Spin-Transfer-FMR Protocol: Apply I(t) = I0 + I_RF·cos(2πν_NW·t); detect rectified voltage ΔV_MR via lock-in technique.
  8. Magnetic Field Calibration: Permanent neodymium magnet (D42-N52) on CONEX-TRB25CC motorized stage; calibrated via NV ESR transition frequencies.
  9. Macrospin Simulation: Landau-Lifshitz-Gilbert equation with spin Hall torque; α = 0.02 assumed for parametric threshold matching.
  10. Thermal Transfer Function: COMSOL finite-element simulation of Py/Pt nanowire on diamond substrate across 265 Hz to GHz range.

This research demands ultra-low-roughness electronic-grade single-crystal diamond with shallow, precisely-engineered NV ensembles, plus complex Ti/Au contact metallization. 6CCVD’s manufacturing capabilities directly support these requirements.

  • Optical Grade SCD (Single Crystal Diamond): This research requires electronic-grade CVD diamond with sub-nanometer surface roughness after plasma etching. 6CCVD’s optical-grade SCD substrates (polished to Ra < 1 nm) provide an ideal starting material for NV-host fabrication.
  • Custom NV-Doped Diamond: While this paper used 15N+ implantation to create shallow NVs, 6CCVD can supply diamond with optimized nitrogen concentrations or coordinate with ion-implantation partners for shallow NV layer formation.
  • Custom Metalization: The paper’s Ti(10 nm)/Pt(10 nm) bilayer nanowire and Ti/Au contact pads were deposited via multi-step e-beam and photolithography. 6CCVD’s in-house metalization capabilities (Ti, Pt, Au, Pd, W, Cu) support research customers who need patterned contacts on diamond substrates.
  • Laser Cutting & Dicing: The 8 µm × 417 nm nanowire geometry is defined by lithography, but 6CCVD can provide laser-cut diamond chips in custom dimensions to fit specific experimental stage geometries or cryogenic mounts.
  • Surface Preparation: 6CCVD’s polishing services (Ra < 1 nm for SCD, < 5 nm for inch-size PCD) deliver the smooth surfaces prerequisite for nanofabrication overlay and low NV depth uncertainty.

6CCVD’s in-house PhD engineering team can assist with material selection for quantum-sensing and spintronics projects—including recommendations on diamond grade, NV density, surface termination chemistry, and compatible metallization stacks for Permalloy/Pt bilayer deposition. Whether the goal is spin-transfer torque characterization, magnetic noise thermometry, or NV-based quantum control, 6CCVD provides consultation from substrate specification through to delivery.

For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

The point-like nature and exquisite magnetic field sensitivity of the nitrogen vacancy (NV) center in diamond can provide information about the inner workings of magnetic nanocircuits in complement with traditional transport techniques. Here, we use a single NV in bulk diamond to probe the stray field of a ferromagnetic nanowire controlled by spin transfer (ST) torques. We first report an unambiguous measurement of ST tuned, parametrically driven, large-amplitude magnetic oscillations. At the same time, we demonstrate that such magnetic oscillations alone can directly drive NV spin transitions, providing a potential new means of control. Finally, we use the NV as a local noise thermometer, observing strong ST damping of the stray field noise, consistent with magnetic cooling from room temperature to ∼150 K.