Dielectric Losses in MPCVD Diamonds in the 25–30 and 250–350 GHz Bands Depending on Growth Parameters
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-11-01 |
| Journal | Technical Physics Letters |
| Authors | Б.М. Гарин, V. V. Parshin, Е. А. Серов, А.С. Ніколенко, Yisa Liu |
| Institutions | Institute of Radio-Engineering and Electronics, University of Science and Technology Beijing |
| Citations | 2 |
Abstract
Section titled “Abstract”A complex systematic study of the effect of various parameters of the CVD diamond growth in a microwave plasma (MPCVD diamonds), such as substrate temperature, the chemical composition of a gas mixture, etc., on dielectric losses in two frequency bands (25-30 and 250-350 GHz) for more than ten samples of various series is carried out. A correlation between the values of the losses in these two frequency bands is identified.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2004 - Proceedings of the IEEE MTT-S International Microwave Symposium