Controlling the fluorescence properties of nitrogen vacancy centers in nanodiamonds
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-12-11 |
| Journal | Nanoscale |
| Authors | Christian Laube, Thomas Oeckinghaus, J. Lehnert, Jan Griebel, Wolfgang Knolle |
| Institutions | University of Stuttgart, Leibniz Institute of Surface Engineering |
| Citations | 57 |
Abstract
Section titled āAbstractāControlled enhancement of NV center fluorescence in nanodiamonds <italic>via</italic> control over the formation process and surface parameters.