CVD Diamond Interaction with Fe at Elevated Temperatures
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-12-10 |
| Journal | Materials |
| Authors | S. Zenkin, A. Gaydaychuk, V. Okhotnikov, Stepan Linnik |
| Institutions | National Research Tomsk State University, Tomsk Polytechnic University |
| Citations | 11 |
Abstract
Section titled āAbstractāChemical vapor deposition (CVD) diamond is a prospective thin film material for cutting tools applications due to the extreme combination of hardness, chemical inertness, and thermal conductivity. However, the CVD diamond cutting ability of ferrous materials is strongly limited due to its extreme affinity to iron, cobalt, or nickel. The diamond-iron interaction and the diffusion behavior in this system are not well studied and are believed to be similar to the graphite-iron mechanism. In this article, we focus on the medium-temperature working range of 400-800 °C of a CVD diamond-Fe system and show that for these temperatures etching of diamond by Fe is not as strong as is generally accepted. The starting point of the diamond graphitization in contact with iron was found around 400 °C. Our results show that CVD diamond is applicable for the cutting of ferrous materials under medium-temperature conditions.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2010 - Diamond growth by chemical vapour deposition [Crossref]
- 2004 - Thermo-chemical wear mechanism of diamond tool in machining of ferrous metals [Crossref]
- 2002 - High quality chemical vapor deposition diamond growth on iron and stainless steel substrates [Crossref]
- 2013 - Etching mechanism of diamond by Ni nanoparticles for fabrication of nanopores [Crossref]
- 1998 - Thermochemical polishing of CVD diamond films [Crossref]
- 1993 - Thinning and patterning of CVD diamond films by diffusional reaction [Crossref]
- 1992 - Study on the polishing of chemically vapour deposited diamond film [Crossref]
- 1992 - Massive thinning of diamond films by a diffusion process [Crossref]
- 1993 - Catalytic interaction of Fe, Ni and Pt with diamond films: Patterning applications [Crossref]
- 2007 - The role of chemical wear in machining iron based materials by PCD and PCBN super-hard tool materials [Crossref]