Active Meta-Mirrors
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Authors | David Lidsky, Zhou Yang, Alexander R. Albrecht, Garrett D. Cole, Mansoor SheikāBahae |
| Institutions | University of New Mexico |
| Citations | 1 |
Abstract
Section titled āAbstractāActive mirror structures based on a dielectric high-contrast grating reflector combined with optical gain are proposed. Design parameters are found that work for III-V based compounds on diamond substrates, thus allowing semiconductor disk lasers with kW output power. Preliminary fabrications validates the concept by exhibiting a passive reflectivity ~99%.