Skip to content

Application of Diamond Wire Saw Cutting in Demolition of Large Reinforced Concrete Members

MetadataDetails
Publication Date2019-01-01
JournalE3S Web of Conferences
AuthorsJianhui YI, Tao Liu, Jie Zhou
Citations2

With the rapid development of construction engineering and densely populated of urban buildings, it is impossible to adopt traditional methods for demolition construction due to the constraints of the surrounding environment. This paper combines the demolition engineering practice of the foundation pit support system of Jinyuan International Plaza, expounds the superiority of the application of diamond wire saw cutting in the demolition of large reinforced concrete members, and puts forward the effective construction operation points, which can provide beneficial for similar projects reference.