Dislocation Analysis of CVD Single Crystal Diamond Using Synchrotron White Beam X-Ray Topography
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Journal | Journal of the Korean Institute of Electrical and Electronic Material Engineers |
| Authors | Yeong-Jae Yu, Seong‐Min Jeong, Si‐Young Bae |
| Institutions | Korea Institute of Ceramic Engineering and Technology |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Focus: Non-destructive analysis of crystalline defects (dislocations) in chemical vapor deposition (CVD) single crystal diamond (SCD) using synchrotron white beam X-ray topography (SWBXRT).
- Primary Challenge Addressed: Dislocation density and lattice strain in CVD-grown diamond, which degrade the performance of next-generation power and radio-frequency (RF) devices.
- Key Material Properties Validated: High thermal conductivity (~22 W/cm·K), high breakdown voltage (>10 MV/cm), and high electron mobility (4,500 cm2/Vs) of single crystal diamond.
- Characterization Method: SWBXRT was utilized to map threading edge dislocations (TEDs) and mixed dislocations across the whole wafer surface.
- Key Findings: The analysis successfully identified numerous threading edge dislocations and five mixed dislocations, demonstrating the prevalence of specific defect types in the crystal lattice.
- Implication: Systematic defect characterization is a prerequisite for developing high-purity, low-strain SCD substrates required for high-power and high-frequency applications.
- Ultimate Goal: To lower dislocation density in CVD diamond to enhance yield and reliability in advanced semiconductor device manufacturing.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Material Analyzed | CVD Single Crystal Diamond (SCD) | N/A | Substrate for next-gen power devices |
| Thermal Conductivity | 22 | W/cm·K | Exceptional heat dissipation property |
| Breakdown Voltage | >10 | MV/cm | High-power operation capability |
| Electron Mobility | 4,500 | cm2/Vs | High-speed electron transport |
| RF Cutoff Frequency | 120 | GHz | Demonstrated in diamond FET |
| RF Power Density | 2.1 | W/mm | Measured at 1 GHz frequency |
| Characterization Technique | Synchrotron White Beam X-Ray Topography (SWBXRT) | N/A | Non-destructive defect mapping |
| Primary Defect Type | Threading Edge Dislocations (TEDs) | N/A | Identified extensively across the surface |
| Secondary Defect Type | Mixed Dislocations | Count: 5 | Identified over the whole surface |
| Crystal Orientation | [001] / [100] / [110] | Miller Indices | Reference axes for topography |
| Growth Method Comparison | CVD vs. HPHT | N/A | CVD offers better doping control and high-purity growth |
Key Methodologies
Section titled “Key Methodologies”- Material Selection: Utilized chemical vapor deposition (CVD) single crystal diamond due to its superior capability for controlling doping concentrations and achieving high-purity growth compared to the high pressure high temperature (HPHT) method.
- Defect Mapping: Employed synchrotron white beam X-ray topography (SWBXRT) as a non-destructive technique to characterize internal crystal lattice defects.
- Sample Rotation: The measurement was executed with a 90° rotation to comprehensively map dislocation networks across different crystallographic vectors.
- Crystallographic Alignment: Samples were analyzed along primary axes, specifically [001], [100], and [110] directions, to isolate specific dislocation types.
- Defect Identification: Threading edge dislocations (TEDs) were distinguished from mixed dislocations based on their distinct topographic contrast signatures.
- Analysis Context: Evaluated the strain fields generated by the dislocations, which are known to cause optical birefringence, affect light propagation, and influence luminescent defects (e.g., nitrogen-vacancy centers).
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Addressing the critical challenge of lattice defects and strain in SCD requires manufacturing precision that begins at the substrate level. 6CCVD provides the high-purity material foundation necessary for advanced device fabrication.
- Applicable Materials: To replicate or extend the research into defect characterization and power device fabrication, Optical Grade Single Crystal Diamond (SCD) or High-Purity SCD Substrates are recommended. 6CCVD’s CVD-grown SCD provides the optimal lattice integrity required for SWBXRT analysis and subsequent device processing.
- Customization Potential: The paper highlights the necessity of analyzing specific crystallographic orientations ([001], [100], [110]). 6CCVD offers custom orientation slicing and laser cutting services to deliver substrates tailored precisely to specific experimental geometries, minimizing edge-induced defects that could confound topography results.
- Metalization Capabilities: For subsequent device fabrication steps following defect analysis (e.g., building the FET structures that achieve 120 GHz cutoff frequencies mentioned in the paper), 6CCVD provides internal metalization services. We support custom multi-layer metal stacks including Ti, Pt, and Au contacts directly on your diamond substrates to ensure optimal adhesion and minimal stress on the crystal lattice.
- Dimensional Control: Whether you require ultra-thin membranes for transmission SWBXRT or thick, robust substrates for power electronics, 6CCVD can deliver SCD in custom thicknesses ranging from 0.1 µm to 500 µm, with plate dimensions up to 125mm (PCD). We ensure a pristine surface finish with Ra < 1nm (SCD) to reduce surface-state scattering and leakage currents.
- Engineering Support: Mitigating threading edge dislocations requires a deep understanding of the growth kinetics. Our in-house PhD engineering team can assist with material selection, advising on the optimal boron-doping ratios (via our BDD options) or growth parameters to reduce lattice strain in your specific high-power or RF device applications.
Call to Action: For custom specifications, substrate orientation consulting, or material selection for your next diamond device project, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Single-crystal diamond obtained by chemical vapor deposition (CVD) exhibits great potential for use in next-generation power devices. Low defect density is required for the use of such power devices in high-power operations; however, plastic deformation and lattice strain increase the dislocation density during diamond growth by CVD. Therefore, characterization of the dislocations in CVD diamond is essential to ensure the growth of high-quality diamond. In this work, we analyze the characteristics of the dislocations in CVD diamond through synchrotron white beam X-ray topography. In estimate, many threading edge dislocations and five mixed dislocations were identified over the whole surface.