High-pressure and high-temperature treatment of N-rich B-doped diamonds
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Journal | CrystEngComm |
| Authors | Xinyuan Miao, Liangchao Chen, Hongan Ma, Chao Fang, Longsuo Guo |
| Institutions | Jilin University, State Key Laboratory of Superhard Materials |
| Citations | 10 |
Abstract
Section titled âAbstractâN-rich B-doped single crystal diamonds with different boron additive contents were annealed in conditions of 2.5 GPa and 2300 K.