Study of optical properties of the NV and SiV centres in diamond at high pressures
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-02-12 |
| Journal | Nanosystems Physics Chemistry Mathematics |
| Authors | S. G. Lyapin, I.D. Ilichev, А. П. Новиков, Valery A. Davydov, V. Agafonov |
| Institutions | GREMAN, Matériaux, Microélectronique, Acoustique, Nanotechnologies, Centre National de la Recherche Scientifique |
| Citations | 18 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Research Focus: Photoluminescence (PL) analysis of optically active point defects (color centers) in diamond subjected to extreme hydrostatic pressures.
- Defects Investigated: Nitrogen-Vacancy (NV0, NV−) and Silicon-Vacancy (SiV−) centers.
- Pressure Range: Successful tracking of Zero-Phonon Line (ZPL) shifts up to ~52 GPa using a Diamond Anvil Cell (DAC) with Helium as the pressure-transmitting medium.
- Key Findings: Quantification of ZPL pressure coefficients (α) and quadratic pressure coefficients (β) for SiV−, NV0, and NV− centers at 296 K and 80 K.
- Synthesis Method: High-Pressure High-Temperature (HPHT) treatment (8 GPa, ~1200 °C, 5-10 s exposure) of metal-free growth systems using naphthalene, fluorographite, and tetrakis(trimethylsilyl)silane to yield nano- and submicrometer diamond agglomerates.
- Significance: Provides foundational data for understanding the electronic structure of quantum-relevant defects under stress, crucial for developing pressure/temperature sensors and quantum metrology applications.
- Analytical Output: Established empirical quadratic equations for ZPL energy shifts as a function of pressure, enabling predictable optical tuning.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Max Hydrostatic Pressure | ~52 | GPa | Achievable limit in the DAC setup for tracking SiV− and NV0. |
| Synthesis Pressure | 8 | GPa | HPHT “Toroid” apparatus loading pressure. |
| Synthesis Temperature | ~1200 | °C | Isothermal exposure temperature for diamond formation. |
| Isothermal Exposure Time | 5 - 10 | s | Duration under constant load during HPHT synthesis. |
| Excitation Wavelength | 488 | nm | Ar+ laser line used for PL excitation. |
| Measurement Temperatures | 296 K & 80 K | K | Room temperature and cryogenic (liquid He) conditions. |
| Laser Spot Size | ~5 | µm | Spot size on the sample inside the cryostat. |
| Objective NA | 0.50 | — | Numerical aperture of the confocal microscope. |
| SiV− ZPL Shift (α) | 1.09 (296K), 1.04 (80K) | meV/GPa | Linear pressure coefficient for Silicon-Vacancy centers. |
| SiV− Quadratic Coeff (β) | -5.7 (296K), -5.3 (80K) | meV/GPa2 | Non-linear pressure coefficient for SiV−. |
| NV− ZPL Shift (α) | 5.81 (296K), 5.57 (80K) | meV/GPa | Linear pressure coefficient for Nitrogen-Vacancy (negative) centers. |
| NV− Quadratic Coeff (β) | -25 (296K), -19 (80K) | meV/GPa2 | Non-linear pressure coefficient for NV−. |
| NV0 ZPL Shift (α) | 2.14 (296K), 2.21 (80K) | meV/GPa | Linear pressure coefficient for neutral NV centers. |
| Detection Limit (NV0) | ~40 | GPa | NV0 ZPL becomes undetectable above this threshold. |
Key Methodologies
Section titled “Key Methodologies”- Synthesis Protocol: Cold pressing of initial mixtures into 4 mm diameter, 5 mm height cylindrical samples.
- HPHT Treatment: Placement into graphite containers inside a “Toroid” high-pressure apparatus; loading to 8 GPa followed by heating to ~1200 °C.
- Exposure Phase: Short isothermal exposure for 5 - 10 seconds under constant load.
- Characterization Setup: PL spectra recorded using a 488 nm Ar+ laser.
- Spectroscopy Equipment: Triple-grating spectrometer (Princeton Instruments TriVista 555) equipped with a liquid-nitrogen-cooled CCD detector.
- High-Pressure Cell: Diamond Anvil Cell (DAC) utilized to apply hydrostatic pressure.
- Pressure Calibration: Ruby crystal used as an internal pressure sensor alongside the diamond samples.
- Pressure Medium: Helium gas used to ensure quasi-hydrostatic pressure transmission to the diamond agglomerates.
- Cryogenic Measurement: DAC integrated into an Oxford Instruments OptistatSXM He cryostat for low-temperature (80 K) measurements using an achromatic focusing lens.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”This research highlights the critical need for high-purity, precisely doped single crystal and polycrystalline diamond to study color center physics under extreme conditions. 6CCVD provides the advanced material platforms required to extend these findings.
-
Applicable Materials:
- Optical Grade Single Crystal Diamond (SCD): Essential for replicating DAC experiments or producing free-standing sensors. Our SCD substrates feature ultra-low nitrogen backgrounds, making them ideal for isolating intrinsic SiV− or NV center emissions without the interference seen in HPHT-grown agglomerates.
- Heavy Boron Doped PCD: While this paper uses undoped diamond for defect analysis, our capability to engineer heavily doped conductive diamond allows for the integration of electrodes for in-situ electrical measurements under high pressure.
-
Customization Potential:
- Ion Implantation Services: To replicate or enhance the color center density demonstrated in the HPHT process, 6CCVD can provide custom substrates optimized for nitrogen or silicon ion implantation to create NV and SiV centers with controlled depth profiles.
- Custom Metalization: For advanced DAC or cryostat integration, 6CCVD offers internal metalization capabilities (Ti, Pt, Au, W, Pd, Cu). This allows for the deposition of custom electrode patterns or reflective optical coatings directly onto the diamond surfaces for enhanced PL collection.
- Precision Laser Cutting: We provide custom laser cutting and shaping to achieve non-standard sample dimensions required for unique high-pressure cell geometries, ensuring minimal edge damage.
-
Engineering Support:
- PhD-Level Consultation: Replicating experiments at 50+ GPa requires impeccable material quality to withstand phase transitions without fracturing. Our in-house PhD engineering team can assist in selecting the optimal SCD or PCD grade to ensure structural integrity under extreme hydrostatic loads.
- Application Specifics: Whether your project focuses on quantum metrology, pressure sensing, or biomedical imaging, our team can provide material consultation to match your specific defect center requirements.
-
Call to Action:
- For custom specifications, material consultation, or specific requirements for high-pressure optics research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
We report photoluminescence studies of micro-and nano-sized diamonds with NV 0 , NV -and SiV -centers under hydrostatic pressure up to 50 GPa. Diamonds have been obtained by high-pressure high-temperature (HPHT) treatment of metal-free growth systems based on mixtures of hydrocarbon, fluorocarbon, and silicone-containing organic compounds.