Nonlinear nanophotonics in lithium niobate

MetadataDetails
Publication Date2019-01-01
JournalUR Research (University of Rochester)
AuthorsRui Luo

With the rapid development of integrated photonics, multiple material platforms, including silicon, silica, diamond, silicon nitride, aluminum nitride, and gallium arsenide, have been widely studied for photonic applications on a chip scale. Particularly, integrated platforms have attracted considerable attention in nonlinear optics, due to boosted nonlinear optical interactions induced by the tight optical confinement. Over the past few decades, lithium niobate (LiNbO3 or LN), with its intriguing material properties, has been extensively studied for nonlinear optics. Recent advances in wafer bonding and etching technology have enabled the fabrication of high-quality LN nanophotonic devices, which have the potential for nonlinear optics with high efficiencies and novel functionalities. This thesis is devoted to the development of nonlinear optical applications based on the LN integrated photonic platform. This thesis starts with a discussion of the thermo-optic property of LN, which is essential for realizing and tuning phase matching in nonlinear optical processes. The large thermo-optic birefringence of LN enables the demonstration of a self-referenced temperature sensor based on a microdisk resonator, exhibiting both a high sensitivity and a high resolution. The large thermo-optic birefringence is further exploited to demonstrate thermally tunable second-harmonic generation in an LN nanophotonic waveguide, which simultaneously achieves a large tuning slope and a high conversion efficiency. In order to further increase the efficiency, semi-nonlinear nanophotonic waveguides are proposed and demonstrated as a universal design principle, which offers a large mode overlap by breaking the spatial symmetry of the optical nonlinearity, resulting in extremely efficient optical parametric generation. Optical microresonators are widely employed to enhance nonlinear optical interactions. This thesis continues on to present applications of LN microresonators in nonlinear optics. First, cavity-enhanced secondharmonic generation and difference-frequency generation are demonstrated in an LN microring resonator with modal phase matching. Then, cyclic phase matching, due to the material anisotropy, is utilized in an X-cut LN microdisk to realize spontaneous parametric down-conversion with an extremely large bandwidth. Finally, Kerr frequency comb generation is demonstrated in an LN microring resonator with an optical quality factor of 2.5 million.