Zero-field magnetometry based on nitrogen-vacancy ensembles in diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Authors | Huijie Zheng, Jingyan Xu, Geoffrey Z. Iwata, T. Lenz, Julia Michl |
| Institutions | Johannes Gutenberg University Mainz, University of Science and Technology of China |
| Citations | 3 |
Abstract
Section titled āAbstractāAt zero ambient field, ground state Zeeman sublevels in ensembles of nitrogen-vacancy centers lose first-order sensitivity to magnetic fields as they are mixed by crystal strain and electric fields. To overcome this, we address specific transitions using polarization-selective microwave excitation and perform zero-field magnetometry with a 250 pT/āHz noise floor.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2014 - Reports on Progress in Physics [Crossref]