Creation of Localized NV Center Ensembles in CVD Diamond by Electron Beam Irradiation

MetadataDetails
Publication Date2019-03-01
JournalTechnical Physics Letters
AuthorsС. А. Богданов, А. М. Горбачев, D.B. Radishev, A. L. Vikharev, M. A. Lobaev
InstitutionsInstitute of Applied Physics, P.N. Lebedev Physical Institute of the Russian Academy of Sciences
Citations4

Creation of localized NV center ensembles, produced by irradiation of CVD diamond with nitrogen doped delta-layer with 200 keV electron beam and the subsequent annealing is demonstrated. Results of optical measurements of activated areas at different irradiation doses are presented. Issues concerning defect formation in diamond lattice during the electron beam impact are discussed.