Skip to content

Diamond saw dicing of thulium channel waveguide lasers in monoclinic crystalline films

MetadataDetails
Publication Date2019-03-19
JournalOptics Letters
AuthorsEsrom Kifle, Pavel Loiko, Uwe Griebner, Valentin Petrov, Patrice Camy
InstitutionsCentre National de la Recherche Scientifique, Universitat Rovira i Virgili
Citations12

A surface channel waveguide (WG) laser is produced by diamond saw dicing of a 15 μm thick 10 at. % Tm:KY<sub>1-x-y</sub>Gd<sub>x</sub>Lu<sub>y</sub>(WO<sub>4</sub>)<sub>2</sub> monoclinic double tungstate thin film grown by liquid phase epitaxy on an undoped KY(WO<sub>4</sub>)<sub>2</sub> substrate. The WG propagation losses are 1.1±0.5 dB/cm. When pumped at 802 nm, laser operation is achieved with a maximum output power of 262 mW at 1833 nm with a record slope efficiency of 82.6% (versus the absorbed pump power) in a TE<sub>10</sub> spatial mode (linear laser polarization, E‖N<sub>m</sub>). Diamond saw dicing of double tungstate epitaxies is a promising technology for manufacturing WGs for sensing applications.