Thermal conductance across β-Ga2O3-diamond van der Waals heterogeneous interfaces
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-03-01 |
| Journal | APL Materials |
| Authors | Zhe Cheng, Luke Yates, Jingjing Shi, Marko J. Tadjer, Karl D. Hobart |
| Institutions | United States Naval Research Laboratory, Georgia Institute of Technology |
| Citations | 162 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Problem Addressed: Mitigating severe self-heating in β-Ga2O3 power electronics by integrating them with diamond heat spreaders. Bulk Ga2O3 suffers from low thermal conductivity (10-30 W/m·K), making high-power operation thermally unreliable.
- Interface Characterization: Measured the thermal boundary conductance (TBC) of a van der Waals (vdW) bonded Ga2O3/single crystal diamond (SCD) interface using time-domain thermoreflectance (TDTR).
- Key Achievement: Achieved a TBC of 17 −1.7/+2.0 MW/m2·K, comparable to physical-vapor-deposited metals on diamond, despite the lack of chemical bonding.
- Phonon Transport Modeling: Applied a Landauer approach combined with density functional theory (DFT) to predict that an optimized, defect-free Ga2O3/diamond interface could theoretically support a higher TBC of ~30-60 MW/m2·K.
- Thermal Conductivity Reduction: Observed significant size-dependent reduction in Ga2O3 thermal conductivity when thinned to nano-membranes (e.g., ~10 W/m·K for thin films vs. ~25 W/m·K bulk), emphasizing the need for ultra-thin, low-defect material transfer.
- Device Simulation: Modeled a hypothetical 500 nm Ga2O3 device on diamond, demonstrating that TBC > 200 MW/m2·K is necessary to outperform state-of-the-art SiC substrates at a power density of 10 kW/mm.
- Significance: Establishes foundational data for designing Ga2O3-on-diamond heterogeneous integration, essential for next-generation high-power, high-frequency RF and power switching devices.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Measured Thermal Boundary Conductance (TBC) | 17 −1.7/+2.0 | MW/m2·K | vdW bonded β-Ga2O3 on SCD |
| Theoretical Maximum TBC (Landauer) | ~30 - 60 | MW/m2·K | Ideal, perfect interface prediction |
| Al-Ga2O3 Interface TBC | 44 | MW/m2·K | Reference: Aluminum transducer on Ga2O3 |
| Bulk β-Ga2O3 Thermal Conductivity | 10 - 30 | W/m·K | Orientation dependent |
| Ga2O3 Nano-membrane Thermal Conductivity | ~10 (thin) to ~25 (thick) | W/m·K | Size-dependent reduction observed |
| SCD Thermal Conductivity | > 2000 | W/m·K | Single crystal diamond substrate |
| Ga2O3 Bandgap | 4.8 | eV | Ultra-wide bandgap semiconductor |
| Ga2O3 Critical Electric Field | 8 | MV/cm | Baliga figure of merit 3214x Si |
| Required TBC for High Power Device | > 200 | MW/m2·K | To outperform SiC at 10 kW/mm power density |
| Diamond Substrate Thickness | 500 | µm | Standard SCD substrate |
| Exfoliated Ga2O3 Membrane Thickness | ~500 | nm | Device relevant dimensions |
| Surface RMS Roughness | 3 - 5 | nm | Measured by AFM (both surfaces) |
| TDTR Echo Times | 25, 154, 179 | ps | Al/Ga2O3 and Ga2O3/diamond interfaces |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Used optical-grade single crystal diamond (SCD) substrates (>2000 W/m·K). AFM surface roughness was characterized prior to integration.
- Material Integration: Mechanically exfoliated thin β-Ga2O3 nano-membranes from bulk crystals and transferred them directly onto the SCD substrates to form a vdW interface.
- Transducer Deposition: An aluminum (Al) thin-film transducer was deposited on top of the Ga2O3/diamond stack for optical measurements.
- Thermal Characterization (TDTR): Time-domain thermoreflectance was utilized to measure the TBC. The pump-probe delay times (25 ps, 154 ps, 179 ps) allowed deconvolution of the Al/Ga2O3 and Ga2O3/diamond thermal responses.
- Theoretical Modeling:
- Applied a Landauer approach for phonon transport across the vdW interface.
- Utilized DFT (Vienna Ab initio Simulation Package - VASP) and the Materials Project database for phonon dispersion calculations.
- Used the diffuse mismatch model (DMM) to predict upper bounds for TBC.
- Device Simulation: Performed finite-element thermal modeling of a hypothetical 500 nm Ga2O3 power device to evaluate the impact of varying interface conductance (G) and substrate thermal conductivity (k) on peak temperature and thermal resistance.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”The thermal management challenges highlighted in this paper—specifically the need for ultra-high thermal conductivity substrates and low thermal resistance interfaces—align directly with the core competencies of 6CCVD. We provide the foundational materials required to replicate, validate, and extend this research.
-
Applicable Materials:
- Optical Grade Single Crystal Diamond (SCD): To accurately replicate the TBC measurements, optical-grade SCD substrates (Ra < 1 nm) are essential to minimize phonon scattering at the rough diamond-Ga2O3 boundary. 6CCVD provides custom-sized SCD substrates (0.1 µm to 500 µm thickness) ideal for vdW integration.
- Polycrystalline Diamond (PCD): For applications requiring larger area thermal spreaders or where single-crystal cost is prohibitive, 6CCVD offers PCD plates up to 125mm with thicknesses up to 10mm, delivering bulk thermal conductivities suitable for high-power Ga2O3 packaging.
- Boron-Doped Diamond (BDD): If subsequent research requires diamond with tailored electrical properties (e.g., to act as a heat spreader and ground plane simultaneously for RF devices), our heavy boron-doped PCD/SCD capabilities are directly applicable.
-
Customization Potential:
- Surface Engineering: Achieving theoretical TBC values (>30 MW/m2·K) requires atomically smooth interfaces. 6CCVD’s precision polishing capabilities (Ra < 1nm for SCD, < 5nm for inch-size PCD) provide the pristine surfaces necessary for vdW bonding and reduced phonon boundary scattering.
- Dicing & Shaping: Ga2O3 membrane transfer often requires specific substrate geometries. 6CCVD offers laser cutting and custom dimensions (up to 125mm for PCD) to provide tailored diamond heat spreaders for specific device footprints.
- Future Metallization: For transitioning from vdW contacts to bonded interfaces (which the paper suggests need >200 MW/m2·K for next-gen devices), 6CCVD offers in-house metalization (Ti, Pt, Au, W, Cu) to facilitate robust, high-thermal-conductivity brazed or soldered interfaces.
-
Engineering Support:
- Selecting the correct diamond grade (SCD vs. PCD) and surface finish is critical when targeting specific TBC regimes. 6CCVD’s in-house PhD engineering team can assist researchers in material selection, surface preparation protocols, and thermal modeling support for Ga2O3-on-diamond power electronics projects.
-
Call to Action:
- For custom specifications, specific thermal conductivity requirements, or material consultation regarding diamond integration for wide-bandgap semiconductor devices, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Because of its ultra-wide bandgap, high breakdown electric field, and large-area affordable substrates grown from the melt, β-Ga2O3 has attracted great attention recently for potential applications of power electronics. However, its thermal conductivity is significantly lower than those of other wide bandgap semiconductors, such as AlN, SiC, GaN, and diamond. To ensure reliable operation with minimal self-heating at high power, proper thermal management is even more essential for Ga2O3 devices. Similar to the past approaches aiming to alleviate self-heating in GaN high electron mobility transistors, a possible solution has been to integrate thin Ga2O3 membranes with diamond to fabricate Ga2O3-on-diamond lateral metal-semiconductor field-effect transistor or metal-oxide-semiconductor field-effect transistor devices by taking advantage of the ultra-high thermal conductivity of diamond. Even though the thermal boundary conductance (TBC) between wide bandgap semiconductor devices and a diamond substrate is of primary importance for heat dissipation in these devices, fundamental understanding of the Ga2O3-diamond thermal interface is still missing. In this work, we study the thermal transport across the interfaces of Ga2O3 exfoliated onto a single crystal diamond. The van der Waals bonded Ga2O3-diamond TBC is measured to be 17 −1.7/+2.0 MW/m2 K, which is comparable to the TBC of several physical-vapor-deposited metals on diamond. A Landauer approach is used to help understand phonon transport across a perfect Ga2O3-diamond interface, which in turn sheds light on the possible TBC one could achieve with an optimized interface. A reduced thermal conductivity of the Ga2O3 nano-membrane is also observed due to additional phonon-membrane boundary scattering. The impact of the Ga2O3-substrate TBC and substrate thermal conductivity on the thermal performance of a power device is modeled and discussed. Without loss of generality, this study is not only important for Ga2O3 power electronics applications which would not be realistic without a thermal management solution but also for the fundamental thermal science of heat transport across van der Waals bonded interfaces.