Advancing Electrochemical Microsensor Technologies Using Carbon Nanomaterials for Chronic Dopamine Detection
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-05-01 |
| Journal | ECS Meeting Abstracts |
| Authors | AnāYi Chang, Gaurab Dutta, Shabnam Siddiqui, Prabhu U. Arumugam |
Abstract
Section titled āAbstractāAnalytical microsensors that can reliably detect (bio)molecules in real-time long-term represent one of the greatest challenges for health and environmental monitoring. Developing such microsensors with high sensitivity and selectivity in minimally prepared complex samples is especially difficult. In recent years, the application of nanomaterials and advanced fabrication methods to microsensing has demonstrated major enhancements in key microsensor performance metrics and their ease of integration into miniaturized microelectrode microarray sensor platforms. In this work, we report the electrochemical response of a boron-doped ultrananocrystalline diamond (BDUNCD) microelectrode during long-term dopamine (DA) detection. Specifically, changes to its electrochemical activity and electroactive area due to DA-by products and surface oxidation are studied via scanning electron microscopy, energy dispersive spectroscopy, electrochemical impedance spectroscopy and silver deposition imaging (SDI). The fouling studies with amperometry (AM) and fast scan cyclic voltammetry (FSCV) methods suggest that the microelectrodes are heavily fouled due to poor DA-dopamine-o-quinone cyclization rates followed by a combination of polymer formation and major changes in their surface chemistry. SDI data confirms the presence of the insulating polymer with sparsely-distributed tiny electroactive regions. This resulted in severely distorted DA signals and a 90% loss in signal starting as early as 3 hrs for AM and a 56% loss at 6.5 hrs for FSCV. This underscores the need for cleaning of the fouled microelectrodes if they have to be used long-term. Out of the three in vivo suitable electrochemical cycling cleaning waveforms investigated, the standard waveform (-0.4 V to +1.0 V) provides the best cleaned surface with a fully retained voltammogram shape, no hysteresis, no DA signal loss (a 90±0.72 nA increase) and the smallest charge transfer resistance value of 0.4±0.02 MW even after 6.5 hrs of monitoring. Most importantly, this is the same waveform that is widely used for in vivo detection with carbon fiber microelectrodes. Future work to test these microelectrodes for more than 24 hrs of DA detection is anticipated.