Enhanced electrochemical activity of boron-doped nanocarbon functionalized reticulated vitreous carbon structures for water treatment applications
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2023-11-25 |
| Journal | Diamond and Related Materials |
| Authors | Iwona Kaczmarzyk, Mariusz Banasiak, PaweĹ JakĂłbczyk, MichaĹ Sobaszek, Gabriel StrugaĹa |
| Institutions | Institute of Fluid Flow-Machinery, Polish Academy of Sciences |
| Citations | 1 |
Abstract
Section titled âAbstractâAn extraordinary charge transfer kinetics and chemical stability make a boron-doped diamond (BDD) a promising material for electrochemical applications including wastewater treatment. Yet, with flat geometrical surfaces its scaling options are limited. In this study, the reticulated Vitreous Carbon (RVC) served as a substrate for boron-doped diamondized nanocarbons (BDNC) film growth resulting with complex heterogeneity carbon structures with different morphologies defined by using electron microscopy, microtomography, activation energy studies, and Raman spectroscopy. The proposed modification significantly boosted the electrochemical Fe(CN)63â/4â redox activity. The voltammetry and impedimetric studies revealed its origin as a significantly higher share of electrochemically active sites at the BDNC@RVC electrode (increased by 114 %) combined with enhanced heterogeneous rate constant (2Ă increase up to 8.24¡10â4 cm sâ1). Finally, to establish its applicability for water treatment, the BDNC@RVC was studied as the anode in electrochemical paracetamol decomposition. Boron-enriched nanoarchitecture formed at the RVC electrode surface substantially reduced the oxidation energy barrier manifested as a decrease in activation overpotential by 212 mV, which gave a consequence in a 78 % removal rate (in 4 h, at 0.7 mA cmâ2), 12 % higher than bare RVC and yielding lower amounts of APAP decomposition intermediates.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2010 - Design of ceramic-based cements and putties for bone graft substitution [Crossref]
- 2004 - Reticulated vitreous carbon as an electrode material [Crossref]
- 1991 - Reticulated vitreous carbon-plant tissue composite bioelectrodes [Crossref]
- 2018 - Decolourisation of reactive black-5 at an RVC substrate decorated with PbO2/TiO2 nanosheets prepared by anodic electrodeposition [Crossref]
- 2022 - A review on the use of glassy carbon in advanced technological applications [Crossref]
- 2010 - Reticulated vitreous carbon/polypyrrole composites as electrodes for lithium batteries: preparation, electrochemical characterization and charge-discharge performance [Crossref]
- 2022 - The soluble lead flow battery: image-based modelling of porous carbon electrodes [Crossref]
- 2012 - Characterization of a microbial fuel cell with reticulated carbon foam electrodes [Crossref]
- 2017 - Electrophoretic deposition of carbon nanotube on reticulated vitreous carbon for hexavalent chromium removal in a biocathode microbial fuel cell [Crossref]
- 2006 - Introduction of ion-exchange moieties to reticulated vitreous carbon by direct chemical modification [Crossref]