Diamond Schottky-Diode in a Non-Isolated Buck Converter
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-05-07 |
| Journal | Fraunhofer-Publica (Fraunhofer-Gesellschaft) |
| Authors | Richard Reiner, Verena Zuerbig, Lukas Pinti, Philipp Reinke, Dirk Meder |
Abstract
Section titled āAbstractāThis work presents the in-circuit operation of a diamond Schottky-diode in a non-isolated buck converter for LED applications at mains voltage. A Schottky-diode on boron doped monocrystalline diamond substrate was assembled in an engineering package. Test structures show breakdown voltages up to 1250 V, current densities up to 470 A/cm², a reverse charge below 1 nC and a decreasing on-resistance with increasing temperature. The packaged device was operated with a peak current of 1 A in a 30W buck converter with stable operation at 125°C. The converter achieves a maximum total efficiency of 87% at 14 W.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None