Skip to content

Polycrystalline diamond photonic waveguides realized by femtosecond laser lithography

MetadataDetails
Publication Date2019-06-24
JournalOptical Materials Express
AuthorsHaissam Hanafi, S. Kroesen, Georgia Lewes‐Malandrakis, Christoph E. Nebel, Wolfram H. P. Pernice
InstitutionsFraunhofer Institute for Applied Solid State Physics, University of Münster
Citations13
AnalysisFull AI Review Included
  • Breakthrough in Diamond Photonics: First successful demonstration of Type III depressed cladding waveguides fabricated via femtosecond Direct Laser Writing (DLW) in polycrystalline diamond (PCD), overcoming prior limitations restricted to single crystal diamond (SCD).
  • Target Operational Window: Single-mode waveguiding achieved in the near-infrared telecommunication C-band, with insertion losses ranging from approximately 11.6 dB to 21.1 dB.
  • Material Advantages Highlighted: Use of PCD eliminates nucleation-related defects and surface contamination associated with thin-film diamond, while enabling wafer-scale production at lower cost compared to SCD.
  • Fabrication Innovation: Diamond-graphite phase transitions induced by ultrafast laser pulses create highly localized tensile stress, enabling refractive index modulation without traditional etching.
  • 3D Geometry Enabled: True three-dimensional photonic circuit integration becomes feasible, unlocking applications in quantum photonics, broadband polarizers, and 3D photonic crystals.
  • Scalability Demonstrated: Waveguide core diameters from 20 µm to 30 µm were tested, with optimal performance at 25 µm diameter and 20 nJ pulse energy.
  • Future Quantum Integration: Buried waveguides enable deterministic placement of color defects (e.g., NV centers) for on-chip single-photon networks.
ParameterValueUnitContext
Substrate MaterialPolycrystalline CVD Diamond—Grown via MPCVD at 2.45 GHz
Substrate Thickness300µmAfter chemomechanical polishing
Substrate Dimensions3 × 3mm2Laser-diced pieces
Laser Wavelength800nmTi-sapphire femtosecond system (Coherent Legend)
Pulse Duration115fsFemtosecond regime
Repetition Rate1kHzLow repetition for controlled modification
Numerical Aperture (Objective)0.8NANikon 100x microscope objective
Optimal Pulse Energy20nJBest waveguide performance
High Pulse Energy Threshold25nJInsertion loss increases ~80%
Maximum Tested Pulse Energy30nJ20% higher loss vs. 20 nJ
Optimal Core Diameter25µmSingle-mode guiding achieved
Minimum Core Diameter20µmBelow cutoff, no guiding observed
Maximum Core Diameter30µmTested range upper limit
Operational WavelengthC-band (~1550)nmNear-infrared telecom window
Best Insertion Loss−11.6dBBest-case measured coupling
Worst Insertion Loss−21.1dBHighest measured attenuation
Polarization Supports- and p-polarized—Type III depressed cladding design
Translation Stage PrecisionAerotech ALS 130H—High-precision xyz positioning
  1. Substrate Fabrication:
    • Microwave Plasma Enhanced CVD (MPCVD) at 2.45 GHz in ellipsoidal cavity reactors.
    • 300 µm thick PCD layers grown on silicon templates.
    • Chemomechanical polishing applied for surface quality.
    • Silicon template dissolved; diamond laser-diced into 3 × 3 mm2 pieces.
  2. Direct Laser Writing (DLW) Setup:
    • Femtosecond Ti-sapphire laser (Coherent Legend) at 800 nm central wavelength.
    • 115 fs pulse duration, 1 kHz repetition rate.
    • 100x, 0.8 NA Nikon microscope objective for tight focusing.
  3. Waveguide Formation Mechanism:
    • Non-linear absorption exceeds threshold for permanent structural modification.
    • Diamond-graphite phase transitions generate localized tensile stress.
    • Stress-induced refractive index modulation creates Type III depressed cladding.
  4. Geometry Construction:
    • Single filaments placed on an elliptical pattern to approximate a circular core.
    • Spherical aberration and filamentation cause axially elongated structures.
    • Precise calibration of writing pulse energy vs. addressed depth.
  5. Characterization:
    • Raman spectroscopy to verify structural modifications.
    • Optical insertion loss measurements at telecom wavelengths.
    • Polarization-resolved transmission testing.
Research Requirement6CCVD Capability
300 µm thick PCD substratesPCD thicknesses from 0.1 µm to 500 µm available; substrates up to 10 mm thick
3 × 3 mm2 sample dimensionsCustom laser cutting up to 125 mm wafer-scale PCD plates
Chemomechanical polishing qualityRa < 5 nm polishing for inch-size PCD substrates
Wafer-scale photonic circuitsCustom dimensions and large-area substrates supported
Low surface roughness for waveguide facetsSub-nanometer polishing (Ra < 1 nm for SCD) ensures minimal scattering losses
  • Applicable Materials: For replicating or extending this research, Optical Grade Polycrystalline Diamond (PCD) is the recommended substrate. 6CCVD’s free-standing PCD plates provide the bulk geometry ideal for buried waveguide structures and 3D photonic circuit fabrication. For single-photon emitter integration projects, our SCD substrates with controlled NV or SiV center density are also available.
  • Customization Potential: This research required precise 3 × 3 mm2 dicing from larger CVD diamond wafers. 6CCVD provides custom laser cutting and dicing services to deliver substrates in any required geometry. Additionally, internal metalization capabilities (Au, Pt, Pd, Ti, W, Cu) are available for hybrid photonic-electronic integration or electrode patterning on diamond surfaces.
  • Engineering Support: The waveguide performance is highly sensitive to pulse energy, core diameter, and material inhomogeneity. 6CCVD’s in-house PhD engineering team can assist with material selection—optimizing grain size, surface roughness, and thickness—to maximize refractive index modulation and minimize insertion losses for similar integrated photonics and quantum photonics projects.
  • Scalability Advantage: Unlike SCD-limited prior studies, the PCD platform used here leverages wafer-scale economics. 6CCVD’s capability to produce wafer-sized PCD up to 125 mm provides a direct pathway from laboratory demonstration to commercial-scale photonic circuit production.
  • Quantum Photonics Extension: For projects aiming to incorporate color defects into waveguide networks (as the authors propose), 6CCVD offers Boron-Doped Diamond (BDD) and partner-sourced NV-center diamond materials, with consultation on optimal substrate specifications.

For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

In recent years, the perception of diamond has changed from it being a pure gemstone to a universal high-tech material. In the field of photonics, an increased interest is emerging due to its outstanding optical properties, such as its high refractive index, a spectrally wide transmission window, and high Raman coefficient. Furthermore, the capability to host color defects for room temperature single photon generation makes diamond an attractive platform for quantum photonics. Known as nature’s hardest material, the fabrication and handling of crystalline diamond for integrated optics remains challenging. Here, we report on the fabrication of three-dimensional Type III depressed cladding waveguides in polycrystalline diamond substrates by direct laser writing. Single mode waveguiding is demonstrated in the near-infrared telecommunication C-band. We believe that this enables the fabrication of three-dimensional large-scale photonic circuits, which are essential for advanced classical and quantum diamond photonics.