Hybrid Switch of Correlation and Squeezing Using Resonant and Off-Resonant Excitation Spectrum in Nitrogen-Vacancy Center Diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-08-27 |
| Journal | IEEE photonics journal |
| Authors | Faizan Raza, Al Imran, Abubakkar Khan, Habib Ullah, Siqiang Zhang |
| Institutions | Xiāan Jiaotong University, City University of Hong Kong |
| Citations | 4 |
Abstract
Section titled āAbstractāOptical hybrid communication is one of the key fields of quantum communications, where scientists are focusing to integrate classical and quantum system as single hybrid system. In this regard, we realized optical hybrid switch using second-order fluorescence (FL) and spontaneous parametric four-wave mixing (SPFWM). The hybrid signal contains Stokes and the FL signal which can be distinguished using power of incident beam. In addition, we investigate the resonant and off-resonant excitation spectrum of negatively charged Nitrogen-vacancy (NV<sup>−</sup>) center in diamond. The hybrid switch is realized by results obtained in time domain and intensity noise correlation. The optical hybrid switch can be controlled by power of incident beams. The hybrid index and temporal width contrast of the hybrid switch are about 4 and 90%, respectively.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 1997 - Quantum optics cambridge university press