Homoepitaxy Growth of Single Crystal Diamond under 300 torr Pressure in the MPCVD System

MetadataDetails
Publication Date2019-11-28
JournalMaterials
AuthorsXiwei Wang, Peng Duan, Zhenzhong Cao, Changjiang Liu, Dufu Wang
InstitutionsState Key Laboratory of Crystal Materials, Jinan Institute of Quantum Technology
Citations25

The high-quality single crystal diamond (SCD) grown in the Microwave Plasma Chemical Vapor Deposition (MPCVD) system was studied. The CVD deposition reaction occurred in a 300 torr high pressure environment on a (100) plane High Pressure High Temperature (HPHT) diamond type II a substrate. The relationships among the chamber pressure, substrate surface temperature, and system microwave power were investigated. The surface morphology evolution with a series of different concentrations of the gas mixture was observed. It was found that a single lateral crystal growth occurred on the substrate edge and a systemic step flow rotation from the [100] to the [110] orientation was exhibited on the surface. The Raman spectroscopy and High Resolution X-Ray Diffractometry (HRXRD) prove that the homoepitaxy part from the original HPHT substrate shows a higher quality than the lateral growth region. A crystal lattice visual structural analysis was applied to describe the step flow rotation that originated from the temperature driven concentration difference of the C2H2 ion charged particles on the SCD center and edge.

  1. 2016 - X-ray photoelectron Spectrosc. study of Schottky junctions based on oxygen-/fluorine-terminated (100) diamond [Crossref]
  2. 2017 - Analysis of boron in diamond with UV photoluminescence [Crossref]
  3. 2017 - Quantitative analysis of spectral characteristics and concentration of ensembles of NVāˆ’ centers in diamond [Crossref]
  4. 2016 - Single crystal diamond wafers for high power electronics [Crossref]
  5. 2014 - Diamond synthesis by chemical vapor deposition: The early years [Crossref]
  6. 2009 - Enhanced growth of high quality single crystal diamond by microwave plasma assisted chemical vapor deposition at high gas pressures [Crossref]
  7. 2009 - High quality, large surface area, homoepitaxial MPACVD diamond growth [Crossref]
  8. 2015 - Growth strategies for large and high quality single crystal diamond substrates [Crossref]
  9. 2018 - Three-Dimensional Diamond MPCVD Growth over MESA Structures: A Geometric Model for Growth Sector Configuration [Crossref]
  10. 2016 - Influence of methane concentration on MPCVD overgrowth of 100-oriented etched diamond substrates [Crossref]