Efficient generation of nitrogen vacancy centers by laser writing close to the diamond surface with a layer of silicon nanoballs
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-12-18 |
| Journal | New Journal of Physics |
| Authors | Youying Rong, Zhiping Ju, Qiang Ma, Shikang Liu, Chengda Pan |
| Institutions | East China Normal University, Shanxi University |
| Citations | 13 |
Abstract
Section titled “Abstract”Abstract We proposed a method to effectively fabricate negatively charged nitrogen vacancy (NV − ) centers close to the diamond surface by applying femtosecond laser writing technique. With a thick layer of silicon (Si) nanoballs coated, diamond surface was irradiated by high-fluence femtosecond laser pulses. A large number of NV − centers were created around the laser ablation crater area without thermal annealing. The distribution of the NV − centers was expanded to about 50 μ m away from the crater center. To demonstrate the function of Si nanoballs, we performed the exactly same laser illumination process on the bare region of the sample surface. In this case, only a few NV − centers were generated around ablation crater. At distance of 32 μ m away from crater centers, the NV − density for the case with nanoballs was up to 15.5 times higher compared to the case without nanoballs. Furthermore, we also investigated the influence of laser fluence and pulse number on the NV − density for the case with Si-nanoball layer. Finally, the formation mechanism of NV − centers and the role of Si nanoballs were explained via Coulomb explosion model. The method is demonstrated to be a promising approach to efficiently and rapidly fabricate NV − centers close to the surface of the diamond, which are significant in quantum sensing. Furthermore, the results provide deep insights into complex light-matter interactions.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2011 - Diamond photonics [Crossref]
- 2013 - Quantum photonic devices in single-crystal diamond [Crossref]
- 2011 - Diamond-based single-photon emitters [Crossref]
- 2015 - Fluorescence polarization switching from a single silicon vacancy colour centre in diamond [Crossref]
- 2013 - The nitrogen-vacancy colour centre in diamond [Crossref]
- 2007 - Experimental realization of Wheeler’s delayed-choice gedanken experiment [Crossref]
- 2004 - Experimental open-air quantum key distribution with a single-photon source [Crossref]
- 2010 - Sub-20-nm fluorescent nanodiamonds as photostable biolabels and fluorescence resonance energy transfer donors [Crossref]
- 2011 - Magnetic field imaging with nitrogen-vacancy ensembles [Crossref]
- 2017 - High-sensitivity spin-based electrometry with an ensemble of nitrogen-vacancy centers in diamond [Crossref]