On-Demand Generation of High-Purity Single-Photon Pulses by NV Centers in Diamond under Electrical Excitation
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Journal | Frontiers in Optics / Laser Science |
| Authors | Igor A. Khramtsov, Dmitry Yu. Fedyanin |
| Institutions | Moscow Institute of Physics and Technology |
| Citations | 1 |
Abstract
Section titled āAbstractāWe study for the first time pulsed electrical excitation of NV in diamond and present a strategy to generate strictly one photon per pulse with a probability of 99% at a rate of 100 kHz.