Heterogeneous Integration of Diamond Disk Resonators with Gallium Nitride Photonics
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Journal | OSA Advanced Photonics Congress (AP) 2020 (IPR, NP, NOMA, Networks, PVLED, PSC, SPPCom, SOF) |
| Authors | Jack A. Smith, Charalambos Klitis, P. Hill, Marc Sorel, Erdan Gu |
| Institutions | University of Glasgow, University of Strathclyde |
Abstract
Section titled āAbstractāWe present the integration by high accuracy micro-transfer printing of a freestanding diamond microdisk resonator with gallium nitride (GaN) on sapphire racetrack resonators, measuring respective loaded Q factors of 8 . 8 Ć 10 4 and 3 . 0 Ć 10 4 .