Single-step grown boron doped nanocrystalline diamond-carbon nanograss hybrid as an efficient supercapacitor electrode

MetadataDetails
Publication Date2020-01-01
JournalNanoscale
AuthorsDebosmita Banerjee, Kamatchi Jothiramalingam Sankaran, Sujit Deshmukh, Mateusz Ficek, Chien-Jui Yeh
InstitutionsUniversity of Gdańsk, Imec the Netherlands
Citations34

Boron doped nanocrystalline diamond-carbon nanograss hybrid as an efficient supercapacitor electrode.