Abstract
Section titled “Abstract”Ag induced phonon-phonon coupling effect leads to ultralow thermal conductivity and high thermoelectric performance of diamond-like material Cu<sub>1−x</sub>Ag<sub>x</sub>InTe<sub>2</sub>.