Optimal architecture for diamond-based wide-field thermal imaging

MetadataDetails
Publication Date2020-02-01
JournalAIP Advances
AuthorsRana Tanos, Waseem Akhtar, Serge Monneret, Felipe FƔvaro de Oliveira, Gediminas Seniutinas
InstitutionsCentrale Marseille, Centre National de la Recherche Scientifique
Citations12

Nitrogen-vacancy centers in diamonds possess an electronic spin resonance that strongly depends on temperature, which makes them efficient temperature sensors with sensitivity down to a few mK/Hz. However, the high thermal conductivity of the host diamond may strongly damp any temperature variations, leading to invasive measurements when probing local temperature distributions. In the view of determining possible and optimal configurations for diamond-based wide-field thermal imaging, here, we investigate both experimentally and numerically the effect of the presence of diamonds on microscale temperature distributions. Three geometrical configurations are studied: a bulk diamond substrate, a thin diamond layer bonded on quartz, and diamond nanoparticles dispersed on quartz. We show that the use of bulk diamond substrates for thermal imaging is highly invasive in the sense that it prevents any substantial temperature increase. Conversely, thin diamond layers partly solve this issue and could provide a possible alternative for microscale thermal imaging. Dispersions of diamond nanoparticles throughout the sample appear as the most relevant approach as they do not affect the temperature distribution, although NV centers in nanodiamonds yield lower temperature sensitivities than bulk diamonds.

  1. 2018 - Guiding rules for selecting a nanothermometer [Crossref]
  2. 2018 - Imaging of nonlocal hot-electron energy dissipation via shot noise [Crossref]
  3. 2018 - Numerical and experimental study of near-field heating using tip-enhanced Raman spectroscopy (TERS) [Crossref]
  4. 1999 - Scanning thermal microscopy [Crossref]
  5. 2015 - Scanning thermal microscopy: A review [Crossref]
  6. 2016 - Nanoscale thermal imaging of dissipation in quantum systems [Crossref]
  7. 2005 - Scanning thermal imaging of microelectronic circuits with a fluorescent nanoprobe [Crossref]
  8. 1997 - Scanning confocal optical microscopy and magnetic resonance on single defect centers [Crossref]
  9. 2016 - Wide-field strain imaging with preferentially aligned nitrogen-vacancy centers in polycrystalline diamond [Crossref]
  10. 2019 - Microscopic imaging of the stress tensor in diamond using in situ quantum sensors [Crossref]