AlGaN/GaN high electron mobility transistors on diamond substrate obtained through aluminum nitride bonding technology

MetadataDetails
Publication Date2020-03-30
JournalJournal of Vacuum Science & Technology B Nanotechnology and Microelectronics Materials Processing Measurement and Phenomena
AuthorsMahmoud Abou Daher, Marie Lesecq, Pascal Tilmant, Nicolas Defrance, Michel Rousseau
InstitutionsCentre National de la Recherche Scientifique, Centre de Recherche sur l’HĂ©tĂ©ro-Epitaxie et ses Applications
Citations11

Transfer technology is now becoming very attractive not only for new technologies such as flexible technology but also for solid state technologies when performances are limited by technological barriers that have to be overcome. In this last context, the transfer of high electron mobility transistors (HEMTs) on diamond substrates represents an opportunity to improve the thermal dissipation when the device operates at high radio frequency power levels. Up to now, the technological process for the transfer of these transistors is not detailed in the literature. In this article, the first demonstration of AlGaN/GaN HEMTs on diamond substrates by transfer technology obtained through sputtered aluminum nitride (AlN) layers bonding at low temperature is reported. Devices are first fabricated on AlGaN/GaN epilayers grown on silicon (Si) substrates. Afterward, AlGaN/GaN thin films with devices are released from the Si growth substrate and transferred at 160 °C onto a diamond substrate thanks to an AlN bonding layer. A full description of the transfer technology and all the technological limits and risks are presented. The transferred device provides a maximum DC drain current density IDS Max of 690 mA mm−1 at VGS = 0 V. Furthermore, a cutoff frequency fT of 85 GHz and a maximum oscillation frequency fMAX of 106 GHz are extracted from S-parameter measurements.