Abstract
Section titled āAbstractāAbstract Sulfate is traditionally considered to have retrograde solubility in aqueous solutions. However, our recent hydrothermal diamond-anvil cell (HDAC) experiments have shown that the solubility of Na2SO4 changes from retrograde to prograde in the presence of silica, leading to the formation of sulfate-rich solutions at high temperatures, in line with observations on natural geofluids. In this study, we use synthetic inclusions of fused silica capillary capsules containing saturated Na2SO4 solutions and Na2SO4 crystals to quantitatively investigate the solubility of Na2SO4 at different temperatures in the Na2SO4-SiO2-H2O system. Sulfate concentrations were measured using Raman spectroscopy and calibrated using Cs2SO4 solutions with known concentrations. The solubility of crystalline Na2SO4 dropped slightly when heated from 50 to 225 °C and dramatically from 225 to 313 °C. At 313 °C, the Na2SO4 crystals began to melt, forming immiscible sulfate melt coexisting with the aqueous solution, with or without solid Na2SO4. With the formation of sulfate melt, the solubility of Na2SO4 was reversed to prograde (i.e., solubility increased considerably with increasing temperatures). The solubility of Na2SO4 in the measured solution was significantly higher than that predicted in the absence of SiO2 over the entire temperature range (except for temperatures around 313 °C). This indicates that the presence of SiO2 greatly changes the dissolution behavior of Na2SO4, which may be caused by the formation of a sulfate-silicate intermediates such as Si(OH)4SO42ā. Considering that most crustal fluids are silica-saturated, the solubility curve of Na2SO4 obtained in this study can better reflect the characteristics of geofluids when compared to that of Na2SO4-H2O binary system. At temperatures of 313-425 °C, the solubility of Na2SO4 increases with temperature following the function Csulfate = -3173.7/T + 5.9301, where Csulfate and T represent the solubility of Na2SO4 in mol/kg H2O and temperature in Kelvin, respectively. As an application, this temperature-solubility relationship can be used to evaluate the sulfate contents in fluid inclusions that contain sulfate daughter minerals, based on the temperature of sulfate disappearance obtained from microthermometric analysis. The sulfate concentrations of the ore-forming fluids of the giant Maoniuping carbonatite-related rare earth element (REE) deposit (southwest China) were calculated to be 4.67-4.81 m (mol/kg H2O). These sulfate concentrations were then used as internal standards to calibrate the previously reported semi-quantitative results of laser ablation-inductively coupled plasma-mass spectrometry (LA-ICP-MS) analysis of REE-forming stage fluid inclusions at this deposit. The calculated Ce concentrations in the REE-mineralizing fluid range from 0.42 to 0.49 wt%. The high fluid REE contents suggest that the sulfate-rich fluids are ideal solvents for REE transport. A mass-balance calculation was carried out to evaluate the minimal volume of carbonatite melt that was required for the formation of the giant Maoniuping REE deposit. The result indicates that the carbonatite dikes in the mining area are enough to provide the required fluids and metals, and thus a deep-seated magma chamber is not necessary for ore formation.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2005 - Validation of LA-ICP-MS fluid inclusion analysis with synthetic fluid inclusions. [Crossref]
- 2003 - Package FLUIDS 1. Computer programs for analysis of fluid inclusion data and for modelling bulk fluid properties. [Crossref]
- 1996 - The hydrothermal diamond anvil cell (HDAC) and its applications: Special publication.
- 2007 - Experimental stability of magnesium sulfate hydrates that may be present on Mars. [Crossref]
- 2008 - A new method for synthesizing fluid inclusions in fused silica capillaries containing organic and inorganic material. [Crossref]
- 2020 - Forming sulfate- and REE-rich fluids in the presence of quartz. [Crossref]
- 2016 - The giant Bayan Obo REE-Nb-Fe deposit, China: Controversy and ore genesis. [Crossref]
- 2018 - Indication of bastnasite heavy minerals of Mianxi REE Belt.
- 2003 - Quantitative multi-element analysis of minerals, fluid and melt inclusions by laser-ablation inductively-coupled-plasma mass-spectrometry. [Crossref]
- 1969 - Thermodynamics of hydrothermal systems at elevated temperatures and pressures. [Crossref]