Structural, electrical and mechanical behavior evaluation of palladium doped diamond like carbon thin films
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-06-10 |
| Journal | Journal of Materials Research and Technology |
| Authors | M.I. Khan, Imran Rasheed, Muhammad Abubakr Naeem, Shahbaz Majeed, Ghulam Mustafa |
| Institutions | Qassim University, University of the Punjab |
| Citations | 9 |
Abstract
Section titled āAbstractāPure and palladium (Pd) doped Diamond-like carbon (DLC) thin films have been deposited on glass substrates by using KrF Excimer laser having 248 nm wavelength. The doping concentration of Pd in DLC is 0%, 0.5%, 1.0%, 1.5% and 2.0%. Internal structure, surface morphology, mechanical and electrical characteristics have been carried out by Raman spectroscopy, scanning electron microscopy (SEM), Vickers hardening and four point probes, respectively. Using Raman spectra an improved graphitic behavior of DLC has been observed with increase of Pd contents. Some nano rods were observed at the surface of pure and Pd doped DLC thin films. With increase of Pd concentration in DLC, initially there is an accumulation of particles is observed and when the doping concentration is high i.e. at 2%, cracks formation takes place. The electrical resistivity is decreased by adding Pd into DLC thin films. Further, doping of Pd decreased the hardness of films. These characteristics of Pd doped DLC with increased hardness and electrical conductivity make it potential candidate for electronic devices. Also, doping enhance the graphitic behavior, therefore this material can be used for anti-bacterial and anti- cancerous activities.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2010 - Corrosion behavior of aluminum doped diamond-like carbon thin films in NaCl aqueous solution [Crossref]
- 2015 - Influence of Cr content on the micro-structural and tribological properties of PLD grown nanocomposite DLC-Cr thin films [Crossref]
- 2011 - Fabrication and bio-functionalization of tetrahedral amorphous carbon thin films for bio sensor applications [Crossref]
- 2009 - Effect of plasma energy on enhancing biocompatibility and hemocompatibility of diamond-like carbon film with various titanium concentrations [Crossref]
- 2017 - Preparation of metal-containing diamond-like carbon films by magnetron sputtering and plasma source ion implantation and their properties [Crossref]
- 2019 - Enhancement the graphitic nature of DLC by Au doping and incorporation of 300 keV Ni 2+ ions in DLC thin films
- 2015 - Chromium-doped DLC for implants prepared by laser-magnetron deposition [Crossref]
- 2014 - Synthesis of Ti-doped DLC film on SS304 steels by filtered Cathodic Vacuum Arc (FCVA) technique for tribological improvement [Crossref]
- 2011 - Bias voltage effect on the structure and property of the (Ti: Cu)-DLC films fabricated by cathodic arc plasma [Crossref]
- 2010 - Field emission properties of composite nano-Au/DLC films prepared by CVD technique [Crossref]