Probing thermal magnon current mediated by coherent magnon via nitrogen-vacancy centers in diamond

MetadataDetails
Publication Date2020-07-27
JournalKyoto University Research Information Repository (Kyoto University)
AuthorsDwi Prananto, Yuta Kainuma, Kunitaka Hayashi, Norikazu Mizuochi, Ken‐ichi Uchida
AnalysisFull AI Review Included

Probing Thermal Magnon Current via NV Centers in Diamond: Technical Documentation

Section titled “Probing Thermal Magnon Current via NV Centers in Diamond: Technical Documentation”
  • Core Innovation: Direct detection of thermal magnon current propagating in yttrium iron garnet (YIG) under temperature gradients using nitrogen-vacancy (NV) centers in diamond as quantum sensors.
  • Sensor Platform: Two NV configurations utilized: a bulk diamond beam (2.5 mm × 0.1 mm × 0.1 mm, (110)-oriented) for resonant excitation and ~40 nm nanodiamonds for local, non-resonant sensing.
  • Primary Detection Mechanism: Modification of Rabi oscillation frequencies (ΩR) and longitudinal spin relaxation rates (Γ) of NV centers coupled to magnetostatic surface spin waves (MSSWs) in YIG.
  • Key Performance: Rabi field amplitude bR evolved from 19 ± 0.5 µT (ΔT = +10 K) to 26 ± 0.4 µT (ΔT = -10 K), representing an 18 ± 1% modulation from the ΔT = 0 baseline of 22 ± 0.6 µT.
  • Thermal Magnon Damping Parameter (αth): (10 ± 0.9) × 10-6 for +Bext and (4.3 ± 1) × 10-6 for -Bext, validated against established literature values.
  • Geometric Advantage: NV-based detection succeeds where IR52 spin Hall effect (ISHE) fails, specifically when Bext is perpendicular to both MSSW propagation and ∇T directions.
  • Application Pathway: Establishes a scalable platform for hybridizing spin caloritronics with spin qubit architectures, enabling nanoscale quantum sensing of thermal transport phenomena.

ParameterValueUnitContext
YIG Sample StructureYIG (100 µm) / GGG (550 µm) / YIG (100 µm)µmTrilayer, liquid-phase epitaxy grown, 6 mm × 3 mm lateral dimensions
YIG Lateral Dimensions6 × 3mm × mmMagnetic insulator substrate for MSSW propagation
Diamond Beam Dimensions2.5 × 0.1 × 0.1mm × mm × mm(110)-oriented, bulk SCD for ensemble NV sensing
NV Ensemble Depth (Beam)up to 70 nm (mean 40 nm)nmBeneath diamond beam surface
Nanodiamond Diameter~40nmAdámas Nanotechnologies, sparse NV population
Gold Antenna Diameter50µmTwo antennas (A, B) for MSSW excitation
Antenna Separation~2mmDistance for MSSW propagation
NV-YIG Surface Distance (Beam)~1µmSeparation for resonant coupling
Applied Magnetic Field (Bext)13-19mTTilt angle φ = 32° to (110) plane
Resonance Matching Frequency2.58 / 2.60 / 2.66GHzNV-MSSW coupling conditions
Microwave Drive Power (PMW)1 (beam) / 1000 (nano)mWSpin-wave excitation amplitude
Temperature Gradient (ΔT)-10 to +10KApplied along YIG longitudinal axis
Effective Temperature Difference (ΔTeff)6.6KOver 2 mm distance at YIG top surface
Base Temperature Variation< 1.5KConfirmed negligible contribution to Γ
Gyromagnetic Ratio (γe)2π × 28GHz/TElectron spin constant
Rabi Frequency Change18 ± 1% / 16 ± 2%%At +Bext / -Bext respectively
Longitudinal Relaxation Rate Change37.5% / 23%%Nanodiamond NV at +Bext / -Bext
αth (Rabi, +Bext)(10 ± 0.9) × 10-6—Thermal magnon damping parameter
αth (Rabi, -Bext)(4.3 ± 1) × 10-6—Thermal magnon damping parameter
αth (Relaxation, +Bext)(4.3 ± 1) × 10-6—Cross-validated via T1 measurements
αth (Relaxation, -Bext)(2.5 ± 0.9) × 10-6—Cross-validated via T1 measurements

  • YIG Sample Preparation: Liquid-phase epitaxy-grown trilayer (YIG/GGG/YIG) with bismuth substitution to improve lattice matching; dimensions 6 mm × 3 mm with 100 µm / 550 µm / 100 µm layer thicknesses.
  • MSSW Excitation Setup: Two gold-wire antennas (50 µm diameter) overlaid on upper YIG surface, separated by ~2 mm; microwave power applied via vector network analyzer (Rohde & Schwarz ZVB8) for S-parameter absorption measurements.
  • Magnetic Field Geometry: External field Bext applied along y-axis at tilt angle φ = 32° to the (110) diamond plane, enabling separation of the four NV spin resonance transitions (NV1-NV4) along 〈111〉 directions.
  • Diamond Beam Placement: Positioned at the longitudinal midpoint of upper YIG layer; (110)-oriented to optimize resonant NV-MSSW coupling at ~1 µm separation distance.
  • Nanodiamond Deposition: ~40 nm particles transferred via micropipette to YIG center for local, non-resonant NV spin relaxation measurements.
  • Temperature Gradient Application: Peltier elements at sites A and B controlled independently; ΔT = TA - TB swept from -10 K to +10 K while maintaining constant center temperature.
  • ODMR Measurement Protocol: In-house scanning confocal microscope with green laser initialization and readout; NV ground triplet states (3A2) addressed via ms = 0 ↔ ±1 transitions.
  • Rabi Oscillation Protocol: Laser pulse 1 (initialize to ms = 0) → MW pulse (variable τ for MSSW-driven NV excitation) → Laser pulse 2 (read remaining ms = 0 population).
  • Longitudinal Relaxation Protocol: Laser pulse 1 → dark time τ with concurrent MW drive → Laser pulse 2; relaxation rate Γ extracted via single exponential fitting.

  • Optical Grade Single Crystal Diamond (SCD): The (110)-oriented diamond beam with precisely engineered NV ensemble depth (up to 70 nm, mean 40 nm) is critical for resonant NV-MSSW coupling. 6CCVD’s optical-grade SCD platforms with controlled NV layer formation via ion implantation match the requirements for ensemble NV spin detection in spin caloritronics experiments.
  • Engineered Nanodiamond Powder: The ~40 nm nanodiamonds containing sparse NV centers serve as local quantum sensors for non-resonant magnon detection. 6CCVD supplies nanodiamond powders with tunable NV concentrations for nanoscale thermal transport probing.
  • Custom (110)-Oriented Substrates: The specific crystallographic orientation enables clean separation of the four 〈111〉 NV axis transitions. 6CCVD provides custom-oriented diamond substrates up to 10 mm thickness to support beam-based quantum sensing architectures.
  • Custom Beam Geometry: The 2.5 mm × 0.1 mm × 0.1 mm diamond beam dimensions can be replicated or refined via 6CCVD’s laser cutting services. Custom lengths and cross-sections are available for tailored coupling geometries.
  • Metallization Services: The gold-wire antennas (50 µm diameter) for MSSW excitation can be patterned on diamond surfaces using 6CCVD’s in-house metallization capabilities (Au, Pt, Pd, Ti, W, Cu). Ti/Au or Cr/Au adhesion layers can be deposited for robust RF antenna integration.
  • Thickness Control: SCD thickness from 0.1 µm to 500 µm allows optimization of NV-YIG proximity for enhanced coupling strength; thinner beams reduce the ~1 µm separation barrier noted in the paper.
  • Surface Polishing: Achieving Ra < 1 nm (SCD) is critical for minimizing NV surface noise and maintaining spin coherence in ODMR protocols requiring low decoherence rates.
  • Material Selection Guidance: 6CCVD’s in-house PhD team can assist with NV center density optimization, crystal orientation selection, and doping strategies for spin caloritronics and quantum sensing applications.
  • Application-Specific Consultation: For spin caloritronics, magnon spintronics, and hybrid spin qubit platforms, our engineers can recommend optimal diamond geometries, NV depth profiles, and metallization schemes to maximize MSSW-NV coupling efficiency.
  • Reproducibility Enhancement: If pursuing this research further, 6CCVD can provide standardized diamond beams with well-characterized NV ensemble properties to reduce experimental variability.

For custom specifications, diamond beam fabrication, or material consultation for spin caloritronics and quantum sensing projects, visit 6ccvd.com or contact our engineering team directly. Global shipping is available (DDU default, DDP optional) to support research groups worldwide.

View Original Abstract

Currently, thermally excited magnons are being intensively investigated owing to their potential in computing devices and thermoelectric conversion technologies. We report the detection of thermal magnon current propagating in a magnetic insulator yttrium iron garnet under a temperature gradient using a quantum sensor: electron spins associated with nitrogen-vacancy (NV) centers in diamond. Thermal magnon current was observed as modified Rabi oscillation frequencies of NV spins hosted in a beam-shaped bulk diamond that resonantly coupled with coherent magnon propagating over a long distance. Additionally, using a nanodiamond, alteration in NV spin relaxation rates depending on the applied temperature gradient were observed under a non-resonant NV excitation condition. The demonstration of probing thermal magnon current mediated by coherent magnon via NV spin states serves as a basis for creating a device platform hybridizing spin caloritronics and spin qubits.