A novel highly dispersed tetra-metal nano heterogeneous ozone catalyst derived from microbial adsorption and in situ pyrolysis
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-11-18 |
| Journal | Nanotechnology |
| Authors | Jianping Xie, Wei Keen Fan, Hao Cui, Ning-Ning Feng, G.Z. Wang |
| Institutions | Kunming Institute of Precious Metals, Ministry of Education of the Peopleās Republic of China |
| Citations | 8 |
Abstract
Section titled āAbstractāAbstract In recent years, the pyrolysis of microbial biomasses that adsorb various metal ions has enabled the preparation of carbon-based polymetallic nanomaterials with excellent electrocatalytic and electrical energy storage properties. However, the preparation of ozone catalysts by this technique and the corresponding catalytic oxidation mechanism are still unclear. In this study, an Escherichia coli strain (BL21) was used for tetra-metal (Cu, Fe, Mn and Al) absorption and the obtained microbial biomass was pyrolyzed under the protection of a nitrogen flow at 700 °C and activated at 900 °C to prepare a microbial-char-based tetra-metal ozone catalyst (MCOC). This was used to degrade phenol and coking wastewater and exhibited a strong catalytic capability for coking wastewater, whose chemical oxygen demand removal efficiency of 70.86% is 16.7% higher than that of pure ozone and 14.67%, 7.21% and 3.58% higher than that of three commercial catalysts, respectively. It also improved the efficiency of ozonation for phenol by 33%. The MCOC was characterized by x-ray diffraction, x-ray photoelectron spectroscopy, scanning electron microscopy-energy-dispersive spectroscopy, transmission electron microscopy and other methods. The results demonstrated that the spherical metal nanoparticles had sizes ranging from 3 nm to 7 nm and that crystals of Fe 2 O 3 and Fe 3 P were observed. The study showed that the MCOC promoted the production of more hydroxyl radicals and superoxides from ozone, which attack organics. The oxygen vacancies of the catalyst were also investigated. It was proved that the Lewis acid sites on the surface of metal oxides are the active centers of ozone decomposition. Therefore, this work provides a new method for the synthesis of multi-metal nanocomposites and expands the application of biosynthetic nanomaterials.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2017 - Mechanism of palladium(II) biosorption by Providencia vermicola [Crossref]
- 2018 - Characterization of Pd II biosorption in aqueous solution by Shewanella oneidensis MR-1 [Crossref]
- 2017 - Self-assembled exopolysaccharide nanoparticles for bioremediation and green synthesis of noble metal nanoparticles [Crossref]
- 2017 - Green synthesis of gold nanoparticles coupled with nucleic acid oxidation [Crossref]
- 2011 - Highly reversible lithium storage in Bacillus subtilis-directed porous Co3O4 nanostructures [Crossref]
- 2015 - E. coli-derived carbon with nitrogen and phosphorus dual functionalities for oxygen reduction reaction [Crossref]
- 2018 - Spore carbon from Aspergillus oryzae for advanced electrochemical energy storage [Crossref]
- 2012 - Efficient synthesis of heteroatom (N or S)-doped graphene based on ultrathin craphene oxide-porous silica sheets for oxygen reduction reactions [Crossref]
- 2012 - Sulfur and nitrogen dual-doped mesoporous graphene electrocatalyst for oxygen reduction with synergistically enhanced performance
- 2019 - Bacteria derived biological carbon building robust Li-S batteries [Crossref]