A tesla-order magnetic field effect on all-optical thermometry using photoluminescence spectrum of diamond NV − center
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2020-11-16 |
| Journal | Japanese Journal of Applied Physics |
| Authors | T. Shikama, Takato Watanabe, Mazin Jouda, Masahiro Hasuo |
| Institutions | Kyoto University, Karlsruhe Institute of Technology |
| Citations | 2 |
Abstract
Section titled “Abstract”Abstract The effect of 0-7 T magnetic field on the low wavelength resolution photoluminescence (PL) spectrum used for the all-optical thermometry was investigated. The PL spectra averaged over randomly-oriented color centers at the temperature between 283 and 343 K were measured for the analysis. Approximately 0.1% increase in the PL intensity was found at the longer wavelength side of the zero-phonon line (ZPL) with increasing the field strength. Its effect on the evaluated temperatures using the ZPL relative peak intensity and peak wavelength was less than their uncertainties of 8.7 and 3.7 K at 293 K, respectively.