The fabrication of nanodiamond doped tellurite germanate glass with robust structure and its luminescence

MetadataDetails
Publication Date2020-11-07
JournalJournal of the American Ceramic Society
AuthorsYayan Xu, Haiyong Gan, Zhanling Lu, Renguang Ye, Tanghan Chen
InstitutionsCentre National de la Recherche Scientifique, China Jiliang University
Citations4

Abstract Fluorescence of negative‐charged nitrogen‐vacancy centers in nanodiamond allows applications in quantum metrology, nanoscale sensor, and bioimaging, of utmost relevance to domains from nanotechnologies to biosensing. However, the low color center content and collection efficiency of photons are crucial issues. Although, several studies about coupling nanodiamond into optical waveguides have already been proposed, the search for the most appropriate substance and simplest, most effective method are of keys. In this study, we present a novel nontraditional way to incorporate nanodiamond with increased negative‐charged nitrogen‐vacancy content to 75.48% into tellurite germanate glass. The hybrid glass is stable in structure with predominant TeO 4 trigonal bipyramid. Moreover, the fluorescence intensity is enhanced in composite. Such robust nanodiamond in tellurite germanate glass optical system has the potential to be used for nanoparticle sensing and quantum metrology.