Identification of Natural Type IIa Colourless Diamond with 270 nm Absorption Peak of UV-Visible Spectrum
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-12-12 |
| Journal | Journal of Gems & Gemmology |
| Authors | Jingjing Chen, Yueping Luo |
| Citations | 1 |
Abstract
Section titled āAbstractāIn this paper, the conventional gemmological and spectral characteristics of a type ā ”a colourless diamond sample were analyzed. Gemmological characteristics of the diamond sample were tested by gem microscope; The DiamondViewTM observed the growth structure and photoluminescence of the diamond sample; UV-Vis spectrometer detected the UV-Visible absorption characteristics of the diamond sample; Fourier infrared spectrometer determined the type of the diamond sample; The confocal laser Raman spectrometer and PL-3000 portable laser Raman spectrometer analyzed the characteristic spectra of defects in the diamond sample. Based on the analysis of experimental data, it is concluded that the diamond sample is natural ā ”a type colourless diamond with the characteristic peak at 270 nm in UV-Vis spectrum, which provided complete laboratory appraisal basis, and enriched the instruction and guidance for special type ultraviolet absorption type of natural type ā ”a diamond for daily testing.